Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
PolyOne LubriOne™ NI-30CF/15T-2S Polyamide 610 (Nylon 610) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
PolyOne Nymax™ ND633 GF Black Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D-790 |
PlastiComp Complet® LGF30-PBT Polybutylene Terephthalate, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polybutylene Terephthalate (PBT) with 30% long glass fiber reinforcementInformation pr.. |
|||
Flexural Strength | 221 MPa | 32100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers UTTAP™ SF 50030 GF Polyether Sulfone, 30% Glass Fiber Excellent chemical and electrical resistance, high stiffness, modulus and HDTAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
PolyOne Edgetek® PI-30GF/000 Polyether Imide (PEI) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 221 MPa | 32100 psi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® PI-30GF/000R BLACK Polyether Imide (PEI) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D-790 |
PlastiComp Complet® LCF10/LGF30 - PP Polypropylene, 40% Long Carbon/Glass Fiber Composite PelletsInformation provided by PlastiComp, Inc. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D-790 |
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte.. |
|||
Flexural Strength | 221 MPa | 32100 psi | ISO 178 |
Solvay TECHNYL® C 538XT V30 Natural W PA6, 30% glass filled, DRY Description: Polyamide 6 reinforced with 30% of glass fibers, heat stabilized, with high viscosity and high toughness, for extrusion.Available in: North America Product Applications: This product is.. |
|||
Flexural Strength | 221 MPa | 32100 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFL46ES PA 66 LNP* LUBRICOMP* RFL46ES is a compound based on Nylon 6/6 containing 30% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Heat Stabilized, Easy Molding. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng.. |
|||
Flexural Strength | 221 MPa | 32100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM UC1200 PEI (Asia Pacific) 12% carbon fiber reinforced Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 listing in recognized colors. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and .. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Flexural Strength | 221 MPa | 32100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
Flexural Strength | 221 MPa | 32100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI (Europe-Africa-Middle East) LNP* Stat-kon* Ultem_UC1200 compound is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
Flexural Strength | 221 MPa | 32100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66 LNP* THERMOCOMP* RF0069SZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of th is grade include: Flame Retardant, Heat Stabilized. |
|||
Flexural Strength | 221 MPa | 32100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10 LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Strength | 221 MPa | 32100 psi | ISO 178 |
Polyplastics Duranex® 353RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
Adell AT-37 Nylon 66, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 443 Glass Reinforced, PET Alloy Data provided by the manufacturer, ComAlloy International Company.55% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 758 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has b.. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
Adell AT-17 Nylon 66, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(disconti Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |
|||
Flexural Strength | 221 MPa | 32100 psi | ISO 178 |
Eurostar Star L PA66 15Y D61 PA66, Carbon Filled, Injection Molded Star L PA66 15Y D61 is a PTFE/Silicone Oil Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 221 MPa | 32100 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AFA-4133 V0 Z Polyphthalamide (PPA), Dry
(discontinued **) Amodel AFA-4133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |