Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 141 MPa | 20500 psi | ASTM D790 |
PolyOne Nymax™ GMF 600 A 40 Natural Polyamide 6 (Nylon 6) The Nymax® 600 Series of mineral-reinforced nylon 6 compounds have been specifically developed to provide an excellent balance of physical property performance and durability, with improved surface.. |
|||
Flexural Strength | 141 MPa | 20500 psi | ASTM D790 |
Quadrant EPP Semitron® MDS 100 (ASTM Product Data Sheet) |
|||
Flexural Strength | 141 MPa | 20500 psi | ASTM D790 |
Polymer Resources PPX/NY G10 PPO/Nylon 66 Alloy , 10% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Flexural Strength | 141 MPa | 20500 psi | 2mm/min; ASTM D790 |
Kingfa JH710 G20 Flame Retardant & 20% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Flexural Strength | 141 MPa | 20500 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 9075 PEI High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Flexural Strength | 141 MPa | 20500 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 9075 PEI (Asia Pacific) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Flexural Strength | 141 MPa | 20500 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 9076 PEI Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Flexural Strength | 141 MPa @Temperature 100 °C |
20500 psi @Temperature 212 °F |
2; ISO 178 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Flexural Strength | 141 MPa | 20500 psi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK) AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for.. |
|||
Flexural Strength | 141 MPa | 20500 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM LTX300B PEI Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
Flexural Strength | 141 MPa | 20500 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM LTX300B PEI (Asia Pacific) Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
Flexural Strength | 141 MPa | 20500 psi | ASTM D790 |
Techmer ES HiFill® ABS GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 141 MPa | 20500 psi | ASTM D790 |
Techmer ES Plastiblend® PA6/ABS 1120 GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInformation p.. |
|||
Flexural Strength | 141 MPa | 20500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF0067K PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF0067K is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. |
|||
Flexural Strength | 141 MPa | 20500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester Elastomer LNP THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Glass Fiber, Mineral. Added features of this material include: Flame Retardant. |
|||
Flexural Strength | 141 MPa | 20500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Verton NV0041EV_GY7E147 PC+ABS Preliminary data for 20% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 141 MPa | 20500 psi | ASTM D790 |
SABIC Innovative Plastics NORYL PCN2615H PPE+PS (Asia Pacific) PPE+PS, Noryl, Glass Fiber, Mica, Flame Retardant, UL Grade, Non-Halogen Flame Retaardant, High Flow, |
|||
Flexural Strength | 141 MPa | 20500 psi | ASTM D790 |
Techmer ES Plastiblend® ABS/PBT GF20 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 141 MPa | 20500 psi | |
Cosmic Plastics CP7318 Short Glass Fiber Filled Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Flexural Strength | 141 MPa | 20500 psi | 3.5%; ISO 178 |
GEHR Plastics PPS Polyphenylene Sulfide The linear polyphenylensulfide belongs to the semi-crystalline materials and offers a very high mechanical capacity, thermal and chemical resistance distinguished at the same time, high dimensional .. |
|||
Flexural Strength | 141 MPa | 20500 psi | ASTM D790 |
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 141 MPa | 20500 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 9076 PEI (Asia Pacific) Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |