Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plastiblend® ABS/PBT GF20

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy + GF , Polyester, TP
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® ABS/PBT GF20.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ASTM D792
Water Absorption 0.12 %

@Time 86400 sec
0.12 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 141 MPa
20500 psi
ASTM D790
Flexural Modulus 5.86 GPa
850 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 4.00 J/cm

@Thickness 3.17 mm
7.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 28.8 µm/m-°C
16.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 202 °C
395 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
256 °F
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149
Copyright © lookpolymers.com All Rights Reserved