Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 86.9 MPa | 12600 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging PK8 WHITE 1081 Polyvinyl Chloride, Rigid (PVC, Rigid) The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne |
|||
Flexural Strength | 86.9 MPa | 12600 psi | ASTM D-790 |
Plaskolite Optix® CP - 51 KC General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 86.7 MPa | 12600 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L8230 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Strength | 86.9 MPa | 12600 psi | ASTM D790 |
PolyOne Novablend™ 5035 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | <= 87.0 MPa | <= 12600 psi | ISO 178 |
Polykemi AB POLYasa 2410F High Flow ASA Information provided by Polykemi AB |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Nilit FRIANYL A63 HS-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | <= 87.0 MPa | <= 12600 psi | ISO 178 |
Polykemi AB POLYform POM C M20 Polyoxymethylene Information provided by Polykemi AB |
|||
Flexural Strength | 87.0 MPa | 12600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
Kolon KOCETAL® WR701 Wear Modified Acetal Resin Improved weather resistant and easy flow grade. Applications: Weather resistant products. Information provided by API-Kolon. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY D20009 PC (Asia Pacific) LNP LUBRILOY* D20009 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD200C PC (Asia Pacific) PTFE free polycarbonate compounds with ESD safety and good lubricating perfomrance , suitable for Semiconductor and Hard Disk Drive (HDD) and semicon industry. Added features of this material includ.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
SABIC Innovative Plastics NORYL PX1340 PPE+HIPS (Asia Pacific) PPE+PS MF Filled |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MF742XXH PP LNP* THERMOCOMP* MF742XXH is a compound based on Polypropylene resin containing Glass Fiber and proprietary antimicrobial additives. This product is best suited for touch surfaces in healthcare app.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RB006 PA 66 LNP* THERMOCOMP* RB006 is a compound based on Nylon 66 resin containing 30% Glass Bead. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
Plenco 1508 Polyester, Briquette, Injection Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
Plenco 2408 Phenolic, Granular, Compression Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
Plenco 6343 Phenolic, Granular, Transfer Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Polyplastics Tepcon M90 Acetal-copolymer (POM), General Information provided by PolyPlastics. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
Plenco 4304 Phenolic, Nodular, Injection Molded PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component .. |
|||
Flexural Strength | 87.0 MPa @Strain 3.50 % |
12600 psi @Strain 3.50 % |
ISO 178 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Flexural Strength | 86.8 MPa | 12600 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABSPC 9802 ABS/PC Molding Grade, High Impact, High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 87.0 - 125 MPa | 12600 - 18100 psi | ASTM D790 |
3D Systems Accura® Amethyst™ Plastic for Viper™ SLA® Systems Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. For use with Viper™ SLA® systems.ApplicationsPatterns for use with low and high vulcanizing.. |
|||
Flexural Strength | 86.9 MPa | 12600 psi | GB9341 |
Beijing Evergrow Resources Enylon® Information provided by Beijing Evergrow Resources. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Polyplastics Duracon® M140-44/M140S Acetal Co-polymer (POM), Standard, High flow DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Polyplastics Duracon® M90-45 Acetal Co-polymer (POM), Weather resistance, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |