| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Novablend™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Novablend™ 5035 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 3.24 GPa | 470 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 86.9 MPa | 12600 psi | ASTM D790 |
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
| Izod Impact, Notched | 0.350 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.656 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 67.2 °C @Thickness 1.57 mm |
153 °F @Thickness 0.0618 in |
Annealed; ASTM D648 |
| Flammability, UL94 | V-0 | V-0 | Cell classification 12453(D-1784); UL 94 |
| Oxygen Index | 30 % | 30 % | ISO 4589-2 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | FDA Food Contact, Unspecified Rating | |
| Appearance | Clear/Transparent | |
| Features | Food Contact Acceptable | |
| High Gloss | ||
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Extrusion | |
| Regional Availability | North America | |
| Uses | Profiles | |
| Transparent or Translucent Parts |