| Category | Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced |
| Manufacturer | Polyplastics Co. |
| Trade Name | Tepcon |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polyplastics Tepcon M90 Acetal-copolymer (POM), General.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.41 g/cc | 0.0509 lb/in³ | ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 62.0 MPa | 8990 psi | ISO 527-1, 2 |
| Elongation at Break | 35 % | 35 % | ISO 527-1, 2 |
| Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1, 2 |
| Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
| Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
| Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 120 µm/m-°C <br>@Temperature 20.0 °C |
66.7 µin/in-°F <br>@Temperature 68.0 °F |
ISO 11359-2 |
| CTE, linear, Transverse to Flow | 120 µm/m-°C <br>@Temperature 20.0 °C |
66.7 µin/in-°F <br>@Temperature 68.0 °F |
ISO 11359-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | ISO 75-1, 2 |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | IEC 60093 |
| Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
| Comparative Tracking Index | >= 600 V | >= 600 V | IEC 60112 |