Material Notes:
PPE+PS MF Filled
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Water Absorption 0.13 %

@Time 86400 sec
0.13 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.20 mm
0.0040 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 29.7 g/10 min

@Load 5.00 kg,
Temperature 300 °C
29.7 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
SABIC - Japan Method
Elongation at Break 25 %
25 %
SABIC - Japan Method
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 0.920 J/cm
1.72 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 109 °C

@Thickness 6.40 mm
228 °F

@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94