Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 4304 Phenolic, Nodular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4304 Phenolic, Nodular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component file E40654. 04304 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Water Absorption 0.18 %
0.18 %
ASTM D570
Linear Mold Shrinkage 0.0064 cm/cm
0.0064 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 70
70
ASTM D785
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 0.78 %
0.78 %
ASTM D638
Tensile Modulus 9.90 GPa
1440 ksi
ASTM D638
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
Flexural Modulus 8.50 GPa
1230 ksi
ASTM D790
Compressive Strength 152 MPa
22000 psi
ASTM D695
Izod Impact, Notched 0.214 J/cm
0.401 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.218 J/cm²
1.04 ft-lb/in²
ASTM D256
Impact 140
140
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 190 °C
374 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 178 °C
352 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Oxygen Index 38 %
38 %
ASTM D2863
Shrinkage 0.15 %
0.15 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.40e+11 ohm-cm
1.40e+11 ohm-cm
ASTM D247
Dielectric Constant 6.0
6.0
ASTM D150
Dielectric Strength 9.30 kV/mm
236 kV/in
Step by Step; ASTM D149
11.4 kV/mm
290 kV/in
Short Time; ASTM D149
Dissipation Factor 0.056
0.056
ASTM D150
Arc Resistance 182 sec
182 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638
Users viewing this material also viewed the following: