Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Plaskolite Optix® CP - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ASTM D790 |
Plaskolite West Optix® CA-927 Impact Modified Acrylic Resin Injection Molding Grade Pellets. Better impact strength than CA-924. Excellent surface gloss, optical clarity, and practical toughness. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Flexural Strength | 76.0 MPa | 11000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
M. Holland Company GS411 Polystyrene
(discontinued **) Features: Good Crack Resistance, Crystal, Fast Cycle (Production), Good FlowUses: Disposable Drinkware, Electrical/Electronic ApplicationsApprovals: FDA 21 CFR 177.1640 Processing Method: Extrusio.. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12 LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP AFB42 ABS LNP* THERMOCOMP* AFB42 is a compound based on ABS containing 10% Glass Fiber, 20% Glass Bead. |
|||
Flexural Strength | 75.5 MPa | 11000 psi | ASTM D790 |
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 75.5 MPa | 11000 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® CA-7009 PA/PPE, Antistatic Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 75.5 MPa | 11000 psi | ASTM D790 |
Samsung Cheil Industries Starex® SF-0505H MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6 FR HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | ISO 178 |
Polyram RamShine PV111 Acrylonitrile Butadiene Styrene General purpose ABS for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | dry; ISO 178 |
DSM Novamid® ST220 NAT PA6-I Impact Modified, Injection Molding, Medium Viscosity |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Ensinger Tecatron® XP-64 Compression Molded PPS Compound, 40% Fiberglass Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Ensinger XP-154 Compression Molded PI Compound, 40% Graphite, Premium Grade The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st.. |
|||
Flexural Strength | 76.0 MPa | 11000 psi | 2 mm/min; ISO 178 |
Chi Mei Polylac® PA-757 ABS High gloss, medium impact |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Axiall HHW-191 Rigid PVC, Extrusion Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Axiall 7555 Rigid PVC, Extrusion, White Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn.. |