M. Holland Company GS411 Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company GS411 Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Good Crack Resistance, Crystal, Fast Cycle (Production), Good FlowUses: Disposable Drinkware, Electrical/Electronic ApplicationsApprovals: FDA 21 CFR 177.1640 Processing Method: Extrusion, Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 11 g/10 min

@Load 5.00 kg,
Temperature 200 °C
11 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Tensile Modulus 3.07 GPa
445 ksi
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Izod Impact, Notched 0.187 J/cm
0.350 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 91.7 °C
197 °F
Unannealed; ASTM D648
Vicat Softening Point 98.9 °C
210 °F
ASTM D1525
Descriptive Properties Value Comments
Form Pellets