Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
Manufacturer | SABIC Innovative Plastics (GE Plastics) |
Trade Name | LNP Konduit |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Water Absorption | 0.25 % @Time 86400 sec |
0.25 % @Time 24.0 hour |
SABIC Method |
Moisture Absorption | 0.0400 % | 0.0400 % | 23°C / 50% RH; ISO 62 |
Linear Mold Shrinkage, Flow | 0.0033 cm/cm @Time 86400 sec |
0.0033 in/in @Time 24.0 hour |
ASTM D955 |
Linear Mold Shrinkage, Transverse | 0.0048 cm/cm @Time 86400 sec |
0.0048 in/in @Time 24.0 hour |
ASTM D955 |
Melt Index of Compound | 49 g/10 min @Load 10.0 kg, Temperature 300 °C |
49 g/10 min @Load 22.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 52.0 MPa | 7540 psi | Type I, 5 mm/min; ASTM D638 |
Elongation at Break | 2.0 % | 2.0 % | Type I, 5 mm/min; ASTM D638 |
Tensile Modulus | 7.24 GPa | 1050 ksi | 5 mm/min; ASTM D638 |
Flexural Strength | 76.0 MPa | 11000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Flexural Modulus | 9.04 GPa | 1310 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Izod Impact, Notched | 0.430 J/cm | 0.806 ft-lb/in | ASTM D256 |
Izod Impact, Unnotched | 1.83 J/cm | 3.43 ft-lb/in | ASTM D4812 |
Izod Impact, Unnotched (ISO) | 5.30 - 18.2 kJ/m² | 2.52 - 8.66 ft-lb/in² | ISO R179 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 19.4 µm/m-°C @Temperature 40.0 - 120 °C |
10.8 µin/in-°F @Temperature 104 - 248 °F |
ASTM E 831 |
31.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
17.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
CTE, linear, Transverse to Flow | 45.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.5 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
69.5 µm/m-°C @Temperature 40.0 - 120 °C |
38.6 µin/in-°F @Temperature 104 - 248 °F |
ASTM E 831 | |
Specific Heat Capacity | 1.42 J/g-°C | 0.339 BTU/lb-°F | ASTM C351 |
Thermal Conductivity | 0.990 W/m-K | 6.87 BTU-in/hr-ft²-°F | through-plane, ø80*3mm discs; ISO 22007-2 |
1.20 W/m-K | 8.33 BTU-in/hr-ft²-°F | through-plane, 10*10*3mm sample; ASTM E 1461-07 | |
1.38 W/m-K | 9.58 BTU-in/hr-ft²-°F | in-plane, ø80*3mm discs; ISO 22007-2 | |
2.10 W/m-K | 14.6 BTU-in/hr-ft²-°F | in-plane, ø25*0.4mm disc; ASTM E 1461-07 | |
Deflection Temperature at 1.8 MPa (264 psi) | 199 °C @Thickness 6.40 mm |
390 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
Flammability, UL94 | V-0 @Thickness 1.00 mm |
V-0 @Thickness 0.0394 in |
UL 94 |
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
850 °C | 1560 °F | IEC 60695-2-13 | |
960 °C @Thickness 1.00 - 3.00 mm |
1760 °F @Thickness 0.0394 - 0.118 in |
IEC 60695-2-12 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Dielectric Constant | 4.74 @Frequency 1.00e+9 Hz |
4.74 @Frequency 1.00e+9 Hz |
ASTM ES 7-83 |
Dielectric Strength | >= 10.0 kV/mm @Thickness 1.00 mm |
>= 254 kV/in @Thickness 0.0394 in |
in oil; ASTM D149 |
Dissipation Factor | 0.0077 @Frequency 1.10e+9 Hz |
0.0077 @Frequency 1.10e+9 Hz |
ASTM ES 7-83 |
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |