Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | <= 66.0 MPa | <= 9570 psi | ISO 178 |
Polykemi AB POLYabs N00 LG ABS, Low Gloss Information provided by Polykemi AB |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | 2mm/min; ASTM D790 |
Kingfa FW-620 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmWeather resistanceHeat resistanceGood surfaceApplications:Injection moldingOA deviceChargerTransformerInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Ineos ABS Lustran® 288 ABS, Injection Molding Grade Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® 152WG Capped Wood Grain Thermoplastic Sheet Features:Super tough, durableHigh extensibility, rigidity, abrasion resistance and fire retardancyMore rigid than most thermoplastics, parts deform less when loadedOutstanding resistance to breakage.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® 311 MB Co-Extruded High Impact Fire-Rated Thermoplastic Sheet with Microban® Antimicrobial Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® XD MB 3D Laminate Thermoplastic 3D Laminate for Flat Lamination and Membrane Pressed Uses with Microban® Features:Tough and extremely durableResistant to cracking and chippingSolid, integral color4,000+ custom colorsResistant to a wide range of chemicalsAbrasion resistantFire retardantVery low moisture.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® 321 Co-Extruded High Impact Fire Rated Sheet Features:Metallic cap, black, gray or off-white substrateThickness ranging from 3.18 mm to 8.9 mmTextures: P-3 Velour Matte and P-C Level HaircellImpact resistantEasy to form with good part definiti.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® T MB High Impact Fire Rated Thermoforming Sheet with Microban® Antimicrobial Product Features:Substitute for FR-ABS sheet with competitive pricing but superior cost/performanceHigher breakage resistanceStandard thicknesses from 0.71 mm to 2.36 mmAmong the most rigid of thermoforming.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
SABIC Innovative Plastics NORYL STN15 PPE+HIPS (Asia Pacific) PPE+HIPS Unfilled Auto Interior |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM Test |
Styrolution Luran® S 757 G ASA Luran S 757 G is an easy flowing injection molding ASA grade with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX06403 PP LNP* THERMOCOMP* MX06403 is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM Test |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
SABIC Innovative Plastics NORYL INT1001 PPE+HIPS (Asia Pacific) PPE / HIPS unfilled, high flow for auto interior |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D 790 |
SABIC Innovative Plastics Noryl EBN3001 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | |
Zeon Chemicals Zeonex® 330R Cyclo-Olefin Polymer Zeonex®330R has a lower birefringence than other Zeonex® products. This grade can satisfy market demands in the optical area where low birefringence and high dimensional stability in precision opt.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Unitika M1030DH PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Polyplastics Duranex® CA7200NX Polybutylene Terephthalate (PBT), Antistatic DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Eastar GN119 Copolyester Applications:Personal care and CosmeticsProduct Description: Eastar GN119 Copolyester is a low-I.V. PETG, for sale only in Asia as a high-flow formulation. This product has been GREENGUARD INDOOR .. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Eastar MN006 Copolyester Eastar Copolyester MN006 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester MN006 contains a mold release.Applications/.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | JIS-K-6740 |
Denka VINYKON R4105 PVC, R grade for hard extrusion A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Entec Hypro™ PPH-GF10 Natural Homopolymer Polypropylene, 10% Glass Reinforced Information provided by Entec |
|||
Flexural Strength | 66.0 MPa @Thickness 3.17 mm |
9570 psi @Thickness 0.125 in |
5% strain; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABSPC 7801E ABS/PC Extrusion Grade, High Impact, High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
BASF Ultramid® 8351 HS BK 102 PA6 (Dry) Description: Ultramid 8351 HS BK-102 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughn.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
BASF Ultramid® 8351 HS BK 106 PA6 (Dry) Description: Ultramid 8351 HS BK-106 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughn.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ASTM D-790 |
Axiall 3020 Rigid PVC, Extrusion Georgia Gulf 3020 is a base for use of wood flour up to 40 percent. Impact strength and toughnessFlame retardantChemical resistanceDimensional stabilityInformation provided by Georgia GulfGeorgia G.. |
|||
Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
Unitika BV2120 PA66, Flame Retardant, Conditioned Information provided by Unitika Ltd. |