KYDEX® 321 Co-Extruded High Impact Fire Rated Sheet

Category Polymer , Thermoplastic
Manufacturer KYDEX LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KYDEX® 321 Co-Extruded High Impact Fire Rated Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features:Metallic cap, black, gray or off-white substrateThickness ranging from 3.18 mm to 8.9 mmTextures: P-3 Velour Matte and P-C Level HaircellImpact resistantEasy to form with good part definitionChemical resistantFire retardantExcellent fabrication qualitiesSuggested Applications:Exhibits and DisplaysStore Fixture ComponentsMedical ProductsMachine HousingsInformation provided by Kydex, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
Flexural Strength 66.0 MPa
9570 psi
ASTM D790
Flexural Modulus 2.482 GPa
360.0 ksi
ASTM D790
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 64.4 °C
148 °F
unannealed; ASTM D648
72.9 °C
163 °F
annealed; ASTM D648
Flammability, UL94 V-0
V-0
5VA
5VA