| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
| 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 | |
| Moisture Absorption | 0.200 % | 0.200 % | 50% RH, 24 hrs; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0018 cm/cm <br>@Time 86400 sec |
0.0018 in/in <br>@Time 24.0 hour |
ISO 294 |
| Linear Mold Shrinkage, Transverse | 0.0027 cm/cm <br>@Time 86400 sec |
0.0027 in/in <br>@Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 37.0 MPa | 5370 psi | ISO 527 |
| 39.0 MPa | 5660 psi | ASTM D638 | |
| Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527 |
| 42.0 MPa | 6090 psi | ASTM D638 | |
| Elongation at Break | 3.3 % | 3.3 % | ISO 527 |
| 8.6 % | 8.6 % | ASTM D638 | |
| Elongation at Yield | 2.2 % | 2.2 % | ASTM D638 |
| 2.2 % | 2.2 % | ISO 527 | |
| Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527 |
| 2.99 GPa | 434 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
| 75.0 MPa | 10900 psi | ASTM D790 | |
| Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
| 2.81 GPa | 408 ksi | ASTM D790 | |
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 2.86 J/cm | 5.36 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 78.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
43.3 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 |
| 79.2 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 75.6 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
42.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 96.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
53.3 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 97.0 °C <br>@Thickness 3.20 mm |
207 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 87.0 °C <br>@Thickness 3.20 mm |
189 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | ASTM D257 |
| Surface Resistance | 10 ohm - 1e+05 | 10 ohm - 1e+05 | ASTM D257 |
| Shielding Effectiveness | 40 - 55 dB <br>@Thickness 3.00 mm |
40 - 55 dB <br>@Thickness 0.118 in |
SABIC Method |