Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Eastar MN006 Copolyester

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Eastar
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastar MN006 Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Eastar Copolyester MN006 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester MN006 contains a mold release.Applications/UsesMedical Applications
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength at Break 54.0 MPa
7830 psi
ASTM D638
Tensile Strength, Yield 44.0 MPa
6380 psi
ASTM D638
Elongation at Break 330 %
330 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 1.80 GPa
261 ksi
ASTM D638
Flexural Strength 66.0 MPa
9570 psi
ASTM D790
Flexural Modulus 1.80 GPa
261 ksi
ASTM D790
Izod Impact, Notched 0.700 J/cm

@Temperature -40.0 °C
1.31 ft-lb/in

@Temperature -40.0 °F
ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Puncture Energy 46.0 J
33.9 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
46.0 J

@Temperature -40.0 °C
33.9 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C
163 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
ASTM D648
Optical Properties Metric English Comments
Haze 1.4 %
1.4 %
ASTM D1003
Transmission, Visible 89 %
89 %
Regular Transmittance; ASTM D1003
92 %
92 %
Total Transmittance; ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 249 - 271 °C
480 - 520 °F
Mold Temperature 16.0 - 38.0 °C
60.8 - 100 °F
Drying Temperature 71.0 °C
160 °F
Dry Time 6 hour
6 hour