Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 125 MPa | 18100 psi | |
Plastcom SLOVALEN PH 69 GF 45 PP, 45% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 45% glass fibre, contains the modifier of mechanical properties.Thermo stable. Increased strength in comparison wit.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Premix Premi-Glas® 2203-20 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st.. |
|||
Flexural Strength | 125 MPa | 18100 psi | conditioned, 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibersInformation provided by LANXESS. |
|||
Flexural Strength | 125 MPa | 18100 psi | |
Lehmann & Voss LUVOCOM® 1700-1401 PPO, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Flexural Strength | 125 MPa | 18100 psi | |
Lehmann & Voss LUVOCOM® PA66/TF/40 Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178 |
Solvay TECHNYL® A 225F PA66, DRY Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178 |
Solvay TECHNYL® B 216 Natural D PA66/6, DRY Description: Unreinforced copolyamide 66/6, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 216 offers an excellent combination between impact resistance,.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178 |
Solvay TECHNYL® B 218 Black 21 N PA66/6, DRY Description: Unreinforced copolyamide PA 66/6 , heat stabilized , medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® B 218 offers all of the primary proper.. |
|||
Flexural Strength | 125 MPa | 18100 psi | DIN 54352 |
Schwartz Technical Plastics LAMIGAMID® 510 Polyethylene Terephthalate Application: friction bearings, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D 790 |
SABIC Innovative Plastics Valox® AB9515 ABS+PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 125 MPa | 18100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Flexural Strength | 125 MPa | 18100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN3V is a 30 % glass fibre reinforced material with a HDT/A of 145C according ISO 75. NORYL GFN3V has been approved for potable water applications up to 85C by the UK WFBS according BS 6920 i.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Flexural Strength | 125 MPa | 18100 psi | |
Toyobo ECOVYLOPET® EMC2311 PET Bottle Recycling Grade, 10% Glass Reinforced Features: PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Flexural Strength | 125 MPa | 18100 psi | dry; ISO 178 |
DSM Novamid® 1010GN7-20 BK37 PA6-GF20 FR(30) 0 20% Glass Reinforced, Flame Retardant, Halogen free |
|||
Flexural Strength | >= 125 MPa @Diameter >=100 mm |
>= 18100 psi @Diameter >=3.94 in |
Perpendicular to laminations; IEC 1212-2 4.1 |
Hippe EP GC 41 Woven Glass Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications. Good stability of electrical properties when exposed to high relative humidity.Information provided by Hippe. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Gromax CCP PBT 3010-104 10% Glass Fiber Filled Product Description: PBT glass fiber 10% reinforced injection molding grade.Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and .. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |
|||
Flexural Strength | 125 MPa | 18100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |
|||
Flexural Strength | 125 MPa | 18100 psi | 3.5%; ISO 178 |
GEHR Plastics PPE-30GF Polyphenylene Ether, 30% Glass Fiber
(discontinued **) The 30% glass fiber reinforced PPE has an improved dimensional stability, a very high stiffness and heat resistance that allows further uses. |
|||
Flexural Strength | 125 MPa | 18100 psi | 2 mm/min; ISO 178 |
Hexion Bakelite™ PF 4155 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, good media and temperature resistance. Conditioned Cu-adhesion.Application areas: Commutators (fuel pumps, actuators, starte.. |