| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Novamid® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DSM Novamid® 1010GN7-20 BK37 PA6-GF20 FR(30) 0.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.29 g/cc | 0.0466 lb/in³ | dry; ISO 1183 |
| Moisture Absorption | 2.30 % | 2.30 % | Sim. To ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 38.0 MPa | 5510 psi | cond; ISO 527-1/-2 |
| 77.0 MPa | 11200 psi | dry; ISO 527-1/-2 | |
| Elongation at Break | 4.0 % | 4.0 % | dry; ISO 527-1/-2 |
| 8.0 % | 8.0 % | cond; ISO 527-1/-2 | |
| Tensile Modulus | 3.20 GPa | 464 ksi | cond; ISO 527-1/-2 |
| 5.40 GPa | 783 ksi | dry; ISO 527-1/-2 | |
| Flexural Strength | 60.0 MPa | 8700 psi | cond; ISO 178 |
| 125 MPa | 18100 psi | dry; ISO 178 | |
| Flexural Modulus | 1.50 GPa | 218 ksi | cond; ISO 178 |
| 4.00 GPa | 580 ksi | dry; ISO 178 | |
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
| 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU | |
| Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
| 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1/-3 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 600 V | 600 V | dry; IEC 60112 |