Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.52 MPa @Strain 300 % |
1090 psi @Strain 300 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-2185 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tensile Stress | 7.49 MPa @Strain 0.100 %, Temperature 80.0 °C |
1090 psi @Strain 0.100 %, Temperature 176 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® LW9330 BK851 PBT
(Unverified Data**) Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Tensile Stress | 7.50 MPa @Strain 5.00 %, Temperature 23.0 °C |
1090 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8441 BK316 TPC-ET
(Unverified Data**) Hytrel® HTR8441 is a 55 nom. Shore D thermoplastic polyester elastomer for blow molding. It provides good mechanical properties at high temperature.Information provided by DuPont Performance Polyme.. |
|||
Tensile Stress | 7.50 MPa @Strain 100 % |
1090 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® EM400-BP TPC-ET 34 Shore D, Injection Molding or Extrusion Grade |
|||
Tensile Stress | 7.51 MPa @Strain 0.600 %, Temperature 100 °C |
1090 psi @Strain 0.600 %, Temperature 212 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 7.51 MPa @Strain 16.99 %, Temperature 90.0 °C |
1090 psi @Strain 16.99 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.51 MPa @Strain 16.99 %, Temperature 90.0 °C |
1090 psi @Strain 16.99 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.51 MPa @Strain 147.53 %, Temperature 150 °C |
1090 psi @Strain 147.53 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.49 MPa @Strain 0.190 %, Temperature 150 °C |
1090 psi @Strain 0.190 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo.. |
|||
Tensile Stress | 7.51 MPa @Strain 0.200 %, Temperature -40.0 °C |
1090 psi @Strain 0.200 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D.. |
|||
Tensile Stress | 7.51 MPa @Strain 0.150 %, Temperature 120 °C |
1090 psi @Strain 0.150 %, Temperature 248 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66
(Unverified Data**) Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in.. |
|||
Tensile Stress | 7.54 MPa @Strain 0.0900 %, Temperature -20.0 °C |
1090 psi @Strain 0.0900 %, Temperature -4.00 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |
|||
Tensile Stress | 7.50 MPa @Strain 100 % |
1090 psi @Strain 100 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.52 MPa @Strain 20.0 %, Temperature 100 °C |
1090 psi @Strain 20.0 %, Temperature 212 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Tensile Stress | 7.53 MPa @Strain 17.5 %, Temperature 100 °C |
1090 psi @Strain 17.5 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 7.50 MPa @Strain 5.00 %, Temperature 23.0 °C |
1090 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® G5564 TPC-ET
(Unverified Data**) Hytrel® G5564 is a 55 nom. Shore D, heat stable, plasticiser free high viscosity resin for extrusion; low temperature impact resistance as well as excellent mechanical properties; good hydrocarbon .. |
|||
Tensile Stress | 7.52 MPa @Strain 6.47 %, Temperature 40.0 °C |
1090 psi @Strain 6.47 %, Temperature 104 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 7.54 MPa @Strain 108.54 %, Temperature 160 °C |
1090 psi @Strain 108.54 %, Temperature 320 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 7.53 MPa @Strain 130.82 %, Temperature 120 °C |
1090 psi @Strain 130.82 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.54 MPa @Strain 73.17 %, Temperature 90.0 °C |
1090 psi @Strain 73.17 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.52 MPa @Strain 6.47 %, Temperature 40.0 °C |
1090 psi @Strain 6.47 %, Temperature 104 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.54 MPa @Strain 108.54 %, Temperature 160 °C |
1090 psi @Strain 108.54 %, Temperature 320 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | >= 7.50 MPa @Strain 300 % |
>= 1090 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 382A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |