Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M3800 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M3890 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Novablend™ 9562 Polyvinyl Chloride Alloy (PVC Alloy) Custom MoldingInformation provided by PolyOne |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Oxford Polymers 604-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Europe-Africa-Middle East) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® MC9000 PC+ABS (Asia Pacific) AUTOMOTIVE. PC+ABS; high heat resistant. Ductile at room temperature. Excellent flow.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EM3110R PC Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature -30.0 °C |
12.0 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Europe-Africa-Middle East) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ HC 8210 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon HC 8210 is a high flow, high impact resistance rigid grade offering enhanced chemical resistance for medical device housing applications. It is RoHS compliant with UL V0 and 5VA ratings.Informa.. |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ SF M7010 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ SF M7020 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXE173R PC This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Ravago Manufacturing Americas Hybrid B2035I Polycarbonate + PBT Alloy Available in North America High Impact Resistance Form: PelletsInformation provided by Ravago |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC/ABS-1211P Polycarbonate+ABS, Impact Modified, Platable, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM 7040 MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 1702 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 5727 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® S1100 High Impact PC/ABS alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
DuPont Surlyn® SG201U NC010 Supergloss Molding Alloy Surlyn® SG201U is a modified ionomer resin for applications that require a high gloss, molded in color surface color surface finish directly from the mold. The material is weatherable, durable, an.. |
|||
Izod Impact, Notched | 6.40 J/cm @Temperature 23.0 °C |
12.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Lubrizol Estaloc® 59020 Reinforced Thermoplastic Polyurethane Type: Estaloc® 59020 RETPU is a polyester-type reinforced engineered thermoplastic polyurethane (RETPU).Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers DIAMALOY PC 1812 Impact Modified Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 6.35 mm |
12.0 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9113 White 02 Rigid PVC, Molding, White 02 Georgia Gulf 9113 White 02 is a pre-colored white material with outstanding impact strength and processing properties. It is especially suited for packaging charcoal lighter fluid.Information provi.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.18 mm, Temperature -20.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-CX00 PC+PBT