| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
| Spiral Flow | 119.38 cm | 47.000 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 79 | 79 | ASTM D2240 |
| Tensile Strength, Yield | 41.4 MPa | 6000 psi | Type I, 51 mm/min; ASTM D638 |
| Elongation at Break | 35 % | 35 % | Type I, 51 mm/min; ASTM D638 |
| Tensile Modulus | 2.28 GPa | 331 ksi | Type I, 51 mm/min; ASTM D638 |
| Flexural Strength | 62.7 MPa | 9090 psi | ASTM D790 |
| Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
| Izod Impact, Notched | 1.10 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
2.06 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
| 2.70 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
5.06 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A | |
| 6.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 67.2 °C @Thickness 3.18 mm |
153 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| 71.1 °C @Thickness 3.18 mm |
160 °F @Thickness 0.125 in |
Annealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C @Thickness 3.18 mm |
140 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| 70.0 °C @Thickness 3.18 mm |
158 °F @Thickness 0.125 in |
Annealed; ASTM D648 | |
| UL RTI, Electrical | 90.0 °C | 194 °F | UL 746 |
| UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746 |
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746 |
| Flammability, UL94 | V-0 | V-0 | |
| 5VA | 5VA | ||
| V-0 @Thickness 1.80 mm |
V-0 @Thickness 0.0709 in |
ALL; UL 94 | |
| 5VA @Thickness 1.80 mm |
5VA @Thickness 0.0709 in |
ALL; UL 94 | |
| 5VA @Thickness 1.60 mm |
5VA @Thickness 0.0630 in |
All Colors |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 199 - 210 °C | 390 - 410 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | General Purpose | |
| High Flow | ||
| High Impact Resistance | ||
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Injection Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| RoHS Compliance | RoHS Compliant | |
| Uses | Medical Appliances |