Material Notes:
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 0.10 %
<br>@Time 86400 sec
0.10 %
<br>@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm
<br>@Thickness 3.17 mm
0.0040 in/in
<br>@Thickness 0.125 in
ASTM D955
Melt Flow 25 g/10 min
<br>@Load 5.00 kg,<br> Temperature 265 °C
25 g/10 min
<br>@Load 11.0 lb,<br> Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.7 MPa
9100 psi
ASTM D638
Elongation at Break 110 %
110 %
ASTM D638
Flexural Yield Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
Izod Impact, Notched 1.44 J/cm
<br>@Thickness 3.17 mm,<br> Temperature -40.0 °C
2.70 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature -40.0 °F
ASTM D256
6.41 J/cm
<br>@Thickness 3.17 mm,<br> Temperature 22.8 °C
12.0 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 73.0 °F
ASTM D256
Dart Drop, Total Energy 5.99 J
<br>@Temperature -28.9 °C
4.42 ft-lb
<br>@Temperature -20.0 °F
ASTM D3763
6.14 J
<br>@Temperature 22.8 °C
4.53 ft-lb
<br>@Temperature 73.0 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 81.0 µm/m-°C
45.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 118 °C
245 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB