Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.57 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.94 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LG709W ABS, Low Gloss, Heat Resistance Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Pilllars, Etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG.. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.94 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical TR557 MABS, High Transparency, High Impact Feature: Injection Molding, High Transparency, High ImpactApplication: Electric/Electronic Applications, Copier, Printer etc.CAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.94 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR409E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.94 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.94 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR401T ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9.. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.94 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR407E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Frame, DVD inner part etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by.. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.35 mm |
2.94 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm |
2.94 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HF-3200H PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm |
2.94 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
2.94 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm |
2.94 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® HR-0370F ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.35 mm |
2.94 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0970 LS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.35 mm |
2.94 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0970 MS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.35 mm |
2.94 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® NH-0927 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm |
2.94 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NT-7310 ABS, Unreinforced FR Flame-retardant ABS that can be used in printer frames etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.35 mm |
2.94 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm |
2.94 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HF-3200H PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm |
2.94 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HM-3301GL PC, Glass Filled High Impact PC/GF material that is used for electric and electronic partsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm |
2.94 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
2.94 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
2.94 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.35 mm |
2.94 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0970 MS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.35 mm |
2.94 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® NH-0927 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm |
2.94 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NT-7310 ABS, Unreinforced FR Flame-retardant ABS that can be used in printer frames etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Temperature 0.000 °C |
2.94 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H5211PC High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA, LNE, AENOR,.. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.35 mm |
2.94 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® LH-1070W PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.94 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.94 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR404T ABS, Heat Resistance Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9, and 9001-96-2Information provided by LG Chemical.. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm |
2.94 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HM-3301GL PC, Glass Filled High Impact PC/GF material that is used for electric and electronic partsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.57 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
2.94 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled Information provided by Samsung Cheil Industries. |