Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.480 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.899 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 78761 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.899 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.899 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar GN102 Copolyester
(discontinued **) Eastar GN102 copolyester is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet inhibitor and mold release. Eastar GN102 copolyester will not crystallize and thus offers .. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -30.0 °C |
0.899 ft-lb/in @Temperature -22.0 °F |
injection molded specimen; ASTM D256 |
Phillips Sumika Marlex® AGM-110 Reactor Thermoplastic Polyolefins, Cold Temperature Impact Resistant
(discont Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. .. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -40.0 °C |
0.899 ft-lb/in @Temperature -40.0 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 7304 NC010 Nylon 6
(Unverified Data**) Zytel® 7304 NC010 is a medium viscosity, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
50%RH; ASTM D256 |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -40.0 °C |
0.899 ft-lb/in @Temperature -40.0 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
0.899 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM-D256 |
Ineos ABS Lustran® 256 Extrusion Blending Grade Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi.. |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
0.899 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM-D256 |
Ineos ABS Lustran® ABS 248FC Medical & Food Contact Grade Lustran® ABS 248FC resin is a high-gloss, medium-impact grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of physical properties and has been desi.. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Europe-Africa-Middle East) High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -40.0 °C |
0.899 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite 105E3V36327 Acetate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -20.0 °C |
0.899 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Dow C759-21NA Polypropylene Impact Copolymer Resin DOW C759-21NA Polypropylene Resin is an impact copolymer designed for injection molding with high stiffness, good impact resistance, and good antistatic properties. Key applications include foldabl.. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Dow H349-02 Polypropylene Homopolymer Resin H349-02 Polypropylene Resin intended for use in biaxial oriented (BOPP) film processes. This product can also be used in extrusion and thermoforming applications where improved melt strength is des.. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -40.0 °C |
0.899 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
BASF Ultramid® 8270 HS BK 102 PA6 (Conditioned) Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex.. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -30.0 °C |
0.899 ft-lb/in @Temperature -22.0 °F |
injection molded specimen; ASTM D256 |
Phillips Sumika Marlex® ABF-110 Reactor Thermoplastic Polyolefin, Cold Temperature Impact Resistant
(disconti Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. .. |