Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Tenite 105E3V36327 Acetate Clear, Trsp

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Cellulose Acetate, Molded
Manufacturer Eastman Chemical
Trade Name Tenite
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Eastman Tenite 105E3V36327 Acetate Clear, Trsp.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Cellulosic Acetate 105-27 has a plasticizer level of 27%.Applications/UsesOphthalmic
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Water Absorption 2.3 %
2.3 %
24h Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Collected Volatile Condensable Material 1.8 %
1.8 %
Weight loss on heating, 72hrs, 80°C; ASTM D707
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ASTM D785
Tensile Strength at Break 36.5 MPa
5290 psi
ASTM D638
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Yield Strength 54.5 MPa
7900 psi
ASTM D790
Flexural Modulus 2.137 GPa
310.0 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
<br>@Temperature -40.0 °C
0.899 ft-lb/in
<br>@Temperature -40.0 °F
ASTM D256
1.87 J/cm
<br>@Temperature 23.0 °C
3.50 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 110 - 170 µm/m-°C
<br>@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F
<br>@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Thermal Conductivity 0.170 - 0.330 W/m-K
1.18 - 2.29 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C
163 °F
ASTM D648
Vicat Softening Point 109 °C
228 °F
ASTM D1525
Optical Properties Metric English Comments
Refractive Index 1.46 - 1.49
1.46 - 1.49
n&lt;sub&gt;D&lt;/sub&gt;; ASTM D542
Haze <= 8.5 %
<= 8.5 %
ASTM D1003
Transmission, Visible >= 90 %
<br>@Thickness 1.52 mm
>= 90 %
<br>@Thickness 0.0598 in
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.3 - 3.8
<br>@Frequency 1e+6 Hz
3.3 - 3.8
<br>@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.8 - 18.7 kV/mm
300 - 475 kV/in
ASTM D149
Dissipation Factor 0.010 - 0.15
<br>@Frequency 1e+6 Hz
0.010 - 0.15
<br>@Frequency 1e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Plasticizer, % 27
Soluble Matter Loss, % 0.3
ASTM D570