Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Impact Test | 2.00 J @Temperature 23.0 °C |
1.48 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the America.. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP EX03647H PEI LNP LUBRICOMP* EX03647H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp JL003 PES LNP* Lubricomp* JL003 is a compound based on Polyethersulfone resin containing PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant, Bearing Grade. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT LNP LUBRICOMP* WFL36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS (Asia Pacific) LNP* STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This da.. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DE0069F PC LNP* STAT-KON* DE0069F is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior Molding. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supp.. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DX99873C PC LNP STAT-KON* DX99872C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON REL33 PA 66 LNP STAT-KON* REL33 is a compound based on Nylon 66 resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Impact Test | 2.00 J @Temperature 23.0 °C |
1.48 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP GF006XXZ PSU LNP THERMOCOMP* GF006XXZ is a compound based on Polysulfone resin containing 30% Glass Fiber. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP MX06402H PP LNP* THERMOCOMP* MX06402H is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, Low Extractable. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66 LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66 LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXZ PA 66 LNP THERMOCOMP* RF006XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RX06421S PA 66 LNP* Thermocomp* RX06421S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RX10408H PA 66 LNP* Thermocomp* RX10408H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp WX01910L PBT LNP* Thermocomp* WX01910L is a compound based on Thermoplastic Polyester containing Proprietary Fillers. Characteristics of this grade are: Low Extractable.This data was supplied by SABIC-IP for t.. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC (Asia Pacific) LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supp.. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon DX96690 PC LNP STAT-KON* DX96690 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the America.. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6 LNP* STAT-LOY* PF303 is a Nylon 6 base resin containing 15% Glass Fiber. Added features of this grade includes: Antistat. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RX93402 PA 66 LNP THERMOCOMP* RX93402 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP JF004L PES LNP* THERMOCOMP* JF004L is a compound is based on Polyethersulfone containing 20% Glass Fiber. Characteristics of this grade is: Low Extractible |