| Category | Polymer , Thermoplastic , Polyethersulfone (PES) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP THERMOCOMP |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics LNP THERMOCOMP JF004L PES.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
| Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
| Moisture Absorption | 0.370 % | 0.370 % | 50% RH, 24 hrs; ASTM D570 |
| 0.550 % | 0.550 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0060 cm/cm @Time 86400 sec |
0.0030 - 0.0060 in/in @Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Time 86400 sec |
0.0050 - 0.0070 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 93.0 MPa | 13500 psi | 5 mm/min; ISO 527 |
| 98.0 MPa | 14200 psi | Type I, 5 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 94.0 MPa | 13600 psi | 5 mm/min; ISO 527 |
| 98.0 MPa | 14200 psi | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Break | 2.1 % | 2.1 % | 5 mm/min; ISO 527 |
| 2.9 % | 2.9 % | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Yield | 2.1 % | 2.1 % | 5 mm/min; ISO 527 |
| 2.7 % | 2.7 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 6.36 GPa | 922 ksi | 50 mm/min; ASTM D638 |
| 6.64 GPa | 963 ksi | 1 mm/min; ISO 527 | |
| Flexural Strength | 148 MPa | 21500 psi | 2 mm/min; ISO 178 |
| 149 MPa | 21600 psi | ISO 178 | |
| 152 MPa | 22000 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Yield Strength | 152 MPa | 22000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 6.30 GPa | 914 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 6.30 GPa | 914 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 5.63 J/cm | 10.5 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 32.0 kJ/m² | 15.2 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 216 °C @Thickness 3.20 mm |
421 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 211 °C @Thickness 3.20 mm |
412 °F @Thickness 0.126 in |
unannealed; ASTM D648 |