Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 20 g/10 min @Load 5.00 kg, Temperature 190 °C |
20 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MP 94 High Density Polyethylene - Injection Molding Eraclene MP 94 is a high density polyethylene homopolymer resin (HDPE) with antioxidants, suitable for injection molding application.This resin has a narrow molecular weight distribution and a high .. |
|||
Melt Flow | 20 g/10 min @Load 5.00 kg, Temperature 230 °C |
20 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resi.. |
|||
Melt Flow | 20 g/10 min @Load 5.00 kg, Temperature 265 °C |
20 g/10 min @Load 11.0 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Europe-Africa-Middle East) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 260 °C |
20 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Melt Flow | 20 g/10 min @Load 1.20 kg, Temperature 300 °C |
20 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® EXL1192C PC Copolymer High flow, polycarbonate siloxane copolymer resin. Notched izod ductile to -20C ductility. Enhanced processability compared to standard PC resins. Available in a range of transparent colors.
US .. |
|||
Melt Flow | 20 g/10 min @Load 1.20 kg, Temperature 300 °C |
20 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Melt Flow | 20 g/10 min @Load 1.20 kg, Temperature 300 °C |
20 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Melt Flow | 20 g/10 min @Load 5.00 kg, Temperature 260 °C |
20 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® ML6413 PC (Europe-Africa-Middle East) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Melt Flow | 20 g/10 min @Load 5.00 kg, Temperature 260 °C |
20 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C1100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1100HF is the improved flow version of CYCOLOY C1100 and has been developed to better fill long and complex parts while maintaining still excellent mechanical properties. Its superior flow .. |
|||
Melt Flow | 20 g/10 min @Load 10.0 kg, Temperature 220 °C |
20 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Kingfa HC-110 Modified ABS Features:UL94 HB @ 1.6-3.0mmElectro-platingApplications:Electro-plating partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Flow | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) HB5020 High Density Polyethylene HB-5020 is a high molecular weight high density polyethylene.Applications: extrusion blow moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 250 °C |
20 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 250 °C |
20 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE (Asia Pacific) Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Melt Flow | 20 g/10 min @Load 5.00 kg, Temperature 250 °C |
20 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East) VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 265 °C |
20 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 260 °C |
20 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 260 °C |
20 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Melt Flow | 20 g/10 min @Load 10.0 kg, Temperature 250 °C |
20 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D 1238 |
SABIC Innovative Plastics LNP Thermocomp ML4351HF PC (Asia Pacific) LNP* Thermocomp* ML4351HF is a Light Reflecting Grade.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 20 g/10 min @Load 5.00 kg, Temperature 280 °C |
20 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Asia Pacific) >PPE+PA66-I-TD10 |
|||
Melt Flow | 20 g/10 min @Load 5.00 kg, Temperature 280 °C |
20 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Europe-Africa-Middle East) >PPE+PA66-I-TD10 |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 250 °C |
20 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East) Super high flow FR PBT grade with 15% Glass reinforced |
|||
Melt Flow | 20 g/10 min @Load 3.80 kg, Temperature 200 °C |
20 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East) 10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density. |
|||
Melt Flow | 20 g/10 min @Load 3.80 kg, Temperature 280 °C |
20 g/10 min @Load 8.38 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Melt Flow | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Total MDPE HL 323 Medium Density Polyethylene, Film Resin Medium molecular weight, medium density film resinCharacteristics:Excellent balance of stiffness and impact strengthGood puncture resistanceExcellent compatibility with LDPE and LLDPEGood tensile st.. |
|||
Melt Flow | 20 g/10 min @Load 10.0 kg, Temperature 220 °C |
20 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO-1133 |
Chi Mei Polylac® PA-707 ABS High gloss, high rigid |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 220 °C |
20 g/10 min @Load 4.76 lb, Temperature 428 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients.. |
|||
Melt Flow | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GF4950HS HDPE Blow Molding Polyethylene Copolymer GF4950HS resin is a high-density polyethylene (HDPE), bimodal copolymer offering a combination of good processability and environmental stress crack resistance (ESCR). It is thus recommended for the.. |
|||
Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 260 °C |
20 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Melt Flow | 20 g/10 min @Load 5.00 kg, Temperature 250 °C |
20 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® X6320 PBT+PC X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP.. |