Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products GC30P200-01 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 203RM PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 327UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 327UVE NC010 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Informat.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS6R PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). Contains a higher amount of mold release t.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 275 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 527 °F |
ASTM D3275 |
Solvay Specialty Polymers Halar® 6014F Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Halar® 6014F is a clear, semi-crystalline melt processable fluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in protection and.. |
|||
Melt Flow | 7.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
M. Holland Company AB308LG ABS Acrylonitrile Butadiene Styrene High flowGood impact resistanceHigh stiffnessApplications: Household goodsPackagingInformation provided by M. Holland |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
Hyosung Topilene C600Y PP C600Y Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
|
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical MI-750 MIPS Medium impact |
|||
Melt Flow | 7.0 - 10 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 - 10 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem PRA 0852 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | (Condition G) ASTM D-1238-94a |
Multibase Multi-ABS 3259 Plating Grade Data provided by Multibase. |
|||
Melt Flow | 7.0 g/10 min @Load 6.60 kg, Temperature 337 °C |
7.0 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 343 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 649 °F |
ASTM D1238 |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU) Udel® P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and.. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 280 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 536 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 7.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 2610 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 250 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL LEN2211 PPE+HIPS (Asia Pacific) PPE / HIPS unfilled, FR for LED application |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Styron CALIBREâ„¢ 320 UV Polycarbonate Resin Overview: CALIBREâ„¢ 302 UV polycarbonate resin contains a proprietary UV stabilization package that combines industry standard stabilization against ultraviolet radiation with low plate-out and .. |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FXP 1943 CaC03 and Glass Fiber Hybrid Copolymer Polypropylene DescriptionPolyfort® FXP 1943 is a 20% CAC03 and glass fiber hybrid copolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White 8000 AP Concentrate Based In LDPE DescriptionPOLYBATCH® 8000 AP is an advanced performance white color concentrate containing 70% TiO2 based in LDPE. This product has been specifically engineered to provide improved resistance to .. |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
Total PPC 5571 Polypropylene, Impact Copolymer Injection Molding TOTAL Petrochemicals Polypropylene 5571 is a high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 5571 is characterized by significantly improved impact resistance, while m.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPC 3060 MW5 Polypropylene, Heterophasic Copolymer, Automotive Polypropylene AUTOMOTIVE PPC 3060 MW5 is a heterophasic copolymer with a Melt Flow index of 7 g/10 min.Polypropylene AUTOMOTIVE PPC 3060 MW5 is a high impact copolymer with heat stabilization packag.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPR 6280 Random Copolymer Polypropylene, Cast Film Extrusion Grade Total Petrochemicals PPR 6280 is a random copolymer polypropylene with a melt flow index of 7 g/10 min suitable for the cast extrusion of films with outstanding optical properties and easy heat weld.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers Centrex® 485 Sheet Extrusion Grade Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it.. |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | ASTM D-1238 |
Bapolene® 1057 Polyethylene, Extrusion Coating Bapolene 1057 is low high density polyethylene for high speed extrusion coating applications that require superior adhesion and low neck-in. It complies with US FDA 21CFR177.1520.Applications: Pouc.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Hifax™ ETA-3183EN Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, paintable thermoplastic olefin resin, excellent impact and stiffness balance, good dimensional stability, good paintability, good processabilityA.. |
|||
Melt Flow | 7.0 - 11 g/10 min | 7.0 - 11 g/10 min | ASTM D1238 |
Buckeye Polymers BP RPP 1509 GK BLK Polypropylene, 15% Glass Filled Product Information: 15% glass reinforced polypropyleneProduct Features:Offers improved flex modulus while maintaining a low specific gravity propertyChemically coupled for improvved physical proper.. |