Material Notes:
Overview: CALIBRE™ 302 UV polycarbonate resin contains a proprietary UV stabilization package that combines industry standard stabilization against ultraviolet radiation with low plate-out and discoloration during processing. This will result in less downtime for cleaning and easier processing. This product is designed for co-extrusion as a 50 µm thick layer on standard PC for use in solid and multi-wall sheets. Main Characteristics:Very low plate-outVery high thermal stabilityVery high color stabilityInformation provided by Styron
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Melt Flow 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 72.0 MPa
10400 psi
ISO 527-2/50
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO 527-2/50
Elongation at Break 150 %
150 %
ISO 527-2/50
Elongation at Yield 6.0 %
6.0 %
ISO 527-2/50
Tensile Modulus 2.50 GPa
363 ksi
ISO 527-2/1
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Unannealed; ISO 75-2/A
128 °C
262 °F
Annealed; ISO 75-2/A
Vicat Softening Point 139 °C
282 °F
ISO 306/B50