Material Notes:
Key Features: medium melt flow, medium high modulus, paintable thermoplastic olefin resin, excellent impact and stiffness balance, good dimensional stability, good paintability, good processabilityApplications: automotive claddings and rocker panels, appliques, filler panelsDescription: Hifax ETA-3183EN medium melt flow, paintable, mineral-filled thermoplastic olefin resin has an excellent balance of stiffness, impact resistance, dimensional stability and processability. It was designed to accommodate a variety of automotive exterior ornamentation components.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
Tool, Montell
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D2240
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
Tangent at 0.05 in/min; ASTM D790A
Impact Test 23.0 J

@Temperature -30.0 °C
17.0 ft-lb

@Temperature -22.0 °F
Dynatup Impact, E at Max Load, Ductile; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696