Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 23 g/10 min @Load 3.80 kg, Temperature 230 °C |
23 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 51 HF OG General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 23 g/10 min @Load 3.80 kg, Temperature 230 °C |
23 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 51 HF UVT General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 23 g/10 min @Load 3.80 kg, Temperature 230 °C |
23 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CA - 51 HF OG General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products HP531-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: IP structural componentsAir ducts - distributionA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products HP531-680UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, BJAA Light Parchment Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 23 g/10 min @Load 10.0 kg, Temperature 220 °C |
23 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
Melt Flow | 23 - 27 g/10 min @Load 2.16 kg, Temperature 230 °C |
23 - 27 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers NPP 50-2753 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Melt Flow | 23 g/10 min @Load 3.80 kg, Temperature 230 °C |
23 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A; ASTM D1238 |
Network Polymers PC-1035 Description: Injection Molding Grade Low Gloss PolycarbonateInformation provided by Network Polymers Inc. |
|||
Melt Flow | 23 g/10 min @Load 10.0 kg, Temperature 220 °C |
23 g/10 min @Load 22.0 lb, Temperature 428 °F |
|
PTS Trilac® ABS-MP1000 Metal Plating Grade ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products HP531-679UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, 2B5A Black Ink Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 23 g/10 min | 23 g/10 min | ISO 1133 |
Solvay Engineered Polymers DEXFLEX® 810HSF TPO
(discontinued **) Description: DEXFLEX® 810HSF is a thermoplastic olefinic elastomer (TPO) designed for large molded-in-color automotive exterior applications that require high flow characteristics for excellent pro.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
PolyOne Maxxam® RP81065 HIPS
(discontinued **) Data provided by PolyOne. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 220 °C |
23 g/10 min @Load 4.76 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical KEYFLEX BT 1047D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Flow | 23 g/10 min | 23 g/10 min | ASTM D1238 |
Kolon KOCETAL® GB705 Glass Bead Reinforced Acetal Resin Glass bead added, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 250 °C |
23 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
LG Chemical LUPOY GN5001SF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical LUPOL HM3102A PP+MF10%, High Impact Description: Injection Molding, PP+MF10%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Melt Flow | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 250 °C |
23 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ325 PBT (Asia Pacific) PBT resin, using chemically recycled post consumer PET Bottles. |
|||
Melt Flow | 23 g/10 min @Load 5.00 kg, Temperature 200 °C |
23 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution PS 116 N/L GPPS Styrolution PS 116N/L is a general purpose polystyrene grade with excellent flow properties and improved heat resistance.Excellent flow propertiesHigh heat resistanceInformation provided by Styrolut.. |
|||
Melt Flow | 23 g/10 min @Load 5.00 kg, Temperature 200 °C |
23 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D 1238 |
Styrolution PS 1900 GPPS Foam extrusionVery high flowHigh heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
Melt Flow | 23 g/10 min @Load 10.0 kg, Temperature 240 °C |
23 g/10 min @Load 22.0 lb, Temperature 464 °F |
ISO 1133 |
Styrolution Terblend® N NM-12 ABS/PA6 (Conditioned) Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture.. |
|||
Melt Flow | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Samyang Trirex® 3020IR Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020IR is a high flow grade with added heat stabilizers, separating materials and stain.. |
|||
Melt Flow | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Samyang Trirex® 3020U UV Stable Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020U is a high flow, UV Stable grade.Information provided by Samyang. |
|||
Melt Flow | 23 g/10 min @Load 5.00 kg, Temperature 250 °C |
23 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCD841U PPE-TPE (Asia Pacific) Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Weatherwood 60190U Concentrate Based In LLDPE DescriptionPOLYBATCH® 60190U is a weatherwood color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabi.. |
|||
Melt Flow | 23 g/10 min | 23 g/10 min | |
Zhejiang Juner JEPPB006 High Glossy PP Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Weatherwood 60190U Concentrate Based In LLDPE DescriptionPOLYBATCH® 60190U is a weatherwood color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabi.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Weatherwood 60190U Concentrate Based In LLDPE DescriptionPOLYBATCH® 60190U is a weatherwood color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabi.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ LD 723.28 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 723.28 is a high VA extrusion coating resin, which provides outstanding heat sealability and high clarity. LD 723.28 has a good balance of drawabilty and neck-.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg |
23 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8.5. |
Dow DOWLEX™ IP-22 High Density Polyethylene DOWLEX® IP-22 resin is an improved processing high density polyethylene resin designed for excellent flow, high impact, and moderate stiffness. DOWLEX IP-22 resin balances peak molecular weight wit.. |