Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution PS 1900 GPPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Extrusion Grade
Manufacturer Styrolution
Trade Name PS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution PS 1900 GPPS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Foam extrusionVery high flowHigh heat resistanceFree of zinc and oil additivesInformation provided by Styrolution
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D 955
Melt Flow 23 g/10 min

@Load 5.00 kg,
Temperature 200 °C
23 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 74
74
ASTM D 785
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D 638
Elongation at Break 1.0 %
1.0 %
ASTM D 638
Tensile Modulus 2.96 GPa
430 ksi
ASTM D 638
Flexural Strength 68.9 MPa
10000 psi
ASTM D 790
Flexural Modulus 3.31 GPa
480 ksi
ASTM D 790
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D 638
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D 696
Vicat Softening Point 105 °C

@Load 1.02 kg
221 °F

@Load 2.25 lb
120°C/h; ASTM D 1525
Optical Properties Metric English Comments
Refractive Index 1.59
1.59
Sodium D Line; ASTM D 542
Transmission, Visible 88 - 90 %

@Wavelength 550 nm
88 - 90 %

@Wavelength 550 nm
ASTM D 1003
Electrical Properties Metric English Comments
Dielectric Constant 2.5

@Thickness 1.00 mm,
Frequency 1.00e+6 Hz
2.5

@Thickness 0.0394 in,
Frequency 1.00e+6 Hz
ASTM D 150
Dielectric Strength 19.7 kV/mm
500 kV/in
ASTM D 696
Users viewing this material also viewed the following: