Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Network Polymers NPP 50-2753

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPP 50-2753.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D1505
Melt Flow 23 - 27 g/10 min

@Load 2.16 kg,
Temperature 230 °C
23 - 27 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.9 MPa
3750 psi
chs 2 in/min; ASTM D638
Elongation at Break 250 %
250 %
chs 2 in/min; ASTM D638
Flexural Modulus 1.03 GPa
150 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -113 °C
<= -171 °F
ASTM D746
Users viewing this material also viewed the following: