SABIC Innovative Plastics NORYL WCD841U PPE-TPE (Asia Pacific)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCD841U PPE-TPE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame retardant performance capable of meeting UL VW-1 requirement. 80C application temperature rating as defined by UL 1581. 84 Shore A hardness. Processing typically conducted on standard extrusion equipment. UL 1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Melt Flow 23 g/10 min

@Load 5.00 kg,
Temperature 250 °C
23 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
30S reading; ASTM D2240
Tensile Strength at Break 17.0 MPa
2470 psi
50 mm/min; ISO 527
18.0 MPa
2610 psi
UL 1581
18.0 MPa
2610 psi
Type I, 50 mm/min; ASTM D638
20.0 MPa
2900 psi
after 7days @113°C; UL 1581
Elongation at Break 220 %
220 %
50 mm/min; ISO 527
238 %
238 %
after 7days @113°C; UL 1581
250 %
250 %
Type I, 50 mm/min; ASTM D638
295 %
295 %
UL 1581
Flexural Modulus 0.0900 GPa
13.1 ksi
12.5 mm/min, 100 mm span; ASTM D790
0.0900 GPa
13.1 ksi
12.5 mm/min; ISO 178
Heat Distortion 19 %

@Load 0.250 kg,
Temperature 100 °C
19 %

@Load 0.551 lb,
Temperature 212 °F
UL 1581
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
UL temperature rating; UL 1581
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Oxygen Index 25 %
25 %
ISO 4589
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-13
960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 4.20e+15 ohm-cm
4.20e+15 ohm-cm
ASTM D257
Dielectric Constant 2.6

@Frequency 1.00e+6 Hz
2.6

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 21.5 kV/mm

@Thickness 2.00 mm
546 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.0060

@Frequency 1.00e+6 Hz
0.0060

@Frequency 1.00e+6 Hz
ASTM D150
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Smoke Density on 0.5mm plaque, Flame, Ds, max 133
ASTM E 662
Smoke Density on 0.5mm plaque, Non-flame, Ds, max 170
ASTM E 662
VW-1 Pass
UL 1581