Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | |
Idemitsu Kosan Xarec® EA 543 SPS, 40% Glass Filled |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | |
Idemitsu Kosan Xarec® N WA 5030 SPS, 30% Glass Filled |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | |
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
LG Chemical LUPOS GP-2106F General Purpose ABS, 10% Glass Fiber Reinforced, Weather Resistant, Flame Retardant LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ASTM D995 |
Kotec Carbotex KGN-10MRA Polycarbonate, Flame Retardant, 10% Glass Fiber Reinforced Features: Glass fiber 10% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4 |
Mitsubishi Xantar® G8F 23 UR Polycarbonate-40% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 cm/cm | 0.0030 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistanceInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0045 cm/cm | 0.0030 - 0.0045 in/in | |
LATI Latamid 6 H2 G/65 PA 6, 65% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | |
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0060 cm/cm @Time 86400 sec |
0.0030 - 0.0060 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON AE004 ABS LNP STAT-KON* AE004 is a compound based on ABS resin containing 20% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON AE008XXY ABS LNP* STAT-KON* AE008XXY is a compound based on ABS resin containing 40% Carbon Fiber. Added feature of this material ia: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM UC1200 PEI (Asia Pacific) 12% carbon fiber reinforced Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 listing in recognized colors. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 cm/cm @Thickness 3.17 mm |
0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® HTN GF HS L High Temp Nylon 50% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Heat ResistanceInformation provided by TP Composit.. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS LNP* THERMOCOMP* AF004L is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features include: Exceptional Processing, Non-Brominated & Non-Chlorinated Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0050 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP YH0235AC PE LNP* Thermocomp* YH0235AC is a compound based on Polyester Elastomer containing a metal filler. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON EV008 PEI LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0040 cm/cm @Time 86400 sec |
0.0030 - 0.0040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI (Asia Pacific) LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | ASTM D955 |
Lubrizol Pellethane® 2363-75D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 cm/cm @Thickness 3.20 mm |
0.0030 in/in @Thickness 0.126 in |
|
Unitika A1030GFL45 PA6, 45% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 cm/cm | 0.0030 in/in | |
E-Polymers TEKAPPO® JF201 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® GV-6H PA*-GF60 Product description: Grivory GV-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0060 cm/cm @Time 86400 sec |
0.0030 - 0.0060 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated, Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | |
LATI Latimass 62-01 D025 PA6 Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |