Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | LATI |
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | LATI |
LATI LAPEX A G/10 10% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | Euronil |
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66 Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | ISO 294-4 |
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | ISO 294-4 |
Mitsubishi Xantar® MX 1094 Polycarbonate-9% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | ISO 294-4, 2577 |
Lanxess Durethan® DP 1852/30 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glassfibers, UL V-0 at 0.75 mm (listed),GWIT:775°C at 0,75 mm, GWFI:960°C at 0.75 mm, CTI/A:400, good flowabilityApplication Examples: Hand-held barrel pump housings |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
LATI Lastilac 10 ABS/PC ABS/PC Blend (ABS/PC). Unfilled. Very good surface appearance. High impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
LATI Latamid 6 H2E04 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. Glass fibers. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0080 cm/cm | 0.0055 - 0.0080 in/in | |
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.085 cm/cm | 0.0055 - 0.085 in/in | |
LATI Latiblend 3675 G/10 ABS/PBT, 10% Glass Fiber Reinforced Blend based on Acrylonitrile-Butadiene-Styrene copolymer (ABS) / Polybutylene Terephthalate (PBT). Glass fibers. Good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
LATI Latigloss 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
LATI Latimass 82-03 D080 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0080 cm/cm | 0.0055 - 0.0080 in/in | |
LATI Latiohm 62-08 PD02 G/30 PPA, 30% Glass Fiber Reinforced Dissipative product based on Polyamide 6 (PA6). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
LATI Latishield 36/AR-08A G/17-V0E ABS, Steel/Glass Fiber Reinforced, Flame Retardant EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 cm/cm @Time 86400 sec |
0.0055 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Asia Pacific) LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 cm/cm @Thickness 3.00 mm |
0.0055 in/in @Thickness 0.118 in |
|
Toyobo T-422T Nylon, Mineral-Reinforced Key Feature: High heat distortion and good toughnessInformation provided by Toyobo Co., Ltd |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm @Thickness 3.00 mm |
0.0055 - 0.0075 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
Covestro Bayblend® T50 BBS083 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Goo.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm @Thickness 3.00 mm |
0.0055 - 0.0075 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
Covestro Bayblend® T80 XG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Opt.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm @Thickness 3.00 mm |
0.0055 - 0.0075 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
Covestro Bayblend® T85 SG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Hig.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | LATI |
LATI LARPEEK 50 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | LATI |
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | LATI |
LATI LATISHIELD 90/13-07A-V1 Modified Polyphenylene Oxide (PPOm) Base E.M.I. Shielding Plastic (UL94 V-1)
(di Description: Latishield E.M.I. shielding materials were developed to solve the problem of shielding electromagnetic interferences with plastic components. The answer is a mixture of two different ty.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion .. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0080 cm/cm | 0.0055 - 0.0080 in/in | |
LATI Latilub 95-25GR CE/10 PSU, Mineral Fiber Reinforced, Graphite Filled Self-lubricating product based on Polysulfone (PSU). Graphite. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Linear Mold Shrinkage, Transverse | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
LATI Latimass 82-03 D110 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |