| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | LATI |
|
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | LATI |
|
LATI LAPEX A G/10 10% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**)
Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | Euronil |
|
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66
Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | ISO 294-4 |
|
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | ISO 294-4 |
|
Mitsubishi Xantar® G2F 23 UR Polycarbonate-10% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | ISO 294-4 |
|
Mitsubishi Xantar® MX 1094 Polycarbonate-9% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | ISO 294-4, 2577 |
|
Lanxess Durethan® DP 1852/30 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glassfibers, UL V-0 at 0.75 mm (listed),GWIT:775°C at 0,75 mm, GWFI:960°C at 0.75 mm, CTI/A:400, good flowabilityApplication Examples: Hand-held barrel pump housings
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
|
LATI Lastilac 10 ABS/PC
ABS/PC Blend (ABS/PC). Unfilled. Very good surface appearance. High impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0080 cm/cm | 0.0055 - 0.0080 in/in | |
|
LATI Latamid 6 H2 G/20-V0 PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
|
LATI Latamid 6 H2E04 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. Glass fibers. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
|
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
|
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
|
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
|
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
|
LATI Latigloss 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
|
LATI Latimass 82-03 D080 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
|
LATI Latishield 36/AR-08A G/17-V0E ABS, Steel/Glass Fiber Reinforced, Flame Retardant
EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0055
cm/cm @Time 86400 sec |
0.0055
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Asia Pacific)
LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0055
-
0.0075
cm/cm @Thickness 3.20 mm |
0.0055
-
0.0075
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS
PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0055
cm/cm @Thickness 3.00 mm |
0.0055
in/in @Thickness 0.118 in |
|
|
Toyobo T-422T Nylon, Mineral-Reinforced
Key Feature: High heat distortion and good toughnessInformation provided by Toyobo Co., Ltd
|
|||
| Linear Mold Shrinkage, Transverse |
0.0055
-
0.0075
cm/cm @Thickness 3.00 mm |
0.0055
-
0.0075
in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
|
Covestro Bayblend® M850 XF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Eas..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0055
-
0.0075
cm/cm @Thickness 3.00 mm |
0.0055
-
0.0075
in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
|
Covestro Bayblend® T80 XG PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Opt..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0055
-
0.0075
cm/cm @Thickness 3.00 mm |
0.0055
-
0.0075
in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
|
Covestro Bayblend® T85 SG PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Hig..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | LATI |
|
LATI LARPEEK 50 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | LATI |
|
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 cm/cm | 0.0055 in/in | LATI |
|
LATI LATISHIELD 90/13-07A-V1 Modified Polyphenylene Oxide (PPOm) Base E.M.I. Shielding Plastic (UL94 V-1)
(di
Description: Latishield E.M.I. shielding materials were developed to solve the problem of shielding electromagnetic interferences with plastic components. The answer is a mixture of two different ty..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
|
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0080 cm/cm | 0.0055 - 0.0080 in/in | |
|
LATI Latilub 95-25GR CE/10 PSU, Mineral Fiber Reinforced, Graphite Filled
Self-lubricating product based on Polysulfone (PSU). Graphite. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
|
LATI Latimass 82-03 D110 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
|
|||