Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Polymer Resources PC-G10-[color]-1 Polycarbonate, 10% Glass Reinforced with Mold Release Polycarbonate, 10% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Specific Gravity | 1.27 - 1.29 g/cc | 1.27 - 1.29 g/cc | |
Michelman® VaporBase™ 1065 MVTR primer Description: MVTR primerUsage: VaporBase™ 1065 is a primer designed to be used in tandem with the VaporCoat® series of products. VaporBase™ 1065 works to seal the base substrate allowin.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem 1010KM PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem 1010RF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 9011 PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Europe-Africa-Middle East) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Techmer ES Plaslube® PC-50/TF/13/SI/2 BK3585 Polycarbonate |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 2085-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-ClearForms-PelletsProcessing Method-Extrusi.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. US FDA and EU Food Contact compliant. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem 1010KM PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D 792 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | |
Shin-Etsu Silicones KE-1830 Silicone, RTV Adhesive/Sealant Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ISO 1183 |
Stir SpA Z 70 3 AT (PVC) Application: Molding for beach footwearInformation provided by STIR SpA |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Specific Gravity | 1.27 g/cc @Temperature 25.0 °C |
1.27 g/cc @Temperature 77.0 °F |
|
Dow Corning FS 1265 Fluid, 1000 CST 100% active, fluorosilicone polymer.Information provided by Dow Corning |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Eastman Eastar GN119 Copolyester Applications:Personal care and CosmeticsProduct Description: Eastar GN119 Copolyester is a low-I.V. PETG, for sale only in Asia as a high-flow formulation. This product has been GREENGUARD INDOOR .. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Eastman Eastar MN211 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. MN211 contains a mold release.Application.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | |
Colorite Polymers 8511G-015 (Extrustion), 8512G-015 (Molding) Radiation Sterilizable Vinyl Compound Description: A series of vinyl compounds identified as the Colorite "G" series has been developed to resist discoloration and degradation when subjected to gamma ray sterilization. All components us.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D471; ISO 2781 |
Advanced Polymer Alloys Alcryn® 4680 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 1010M PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |
|||
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
SK Chemicals SKYTHANE® 368D S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |