Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | ASTM D955 |
PolyOne Gravi-Tech™ GRV-NY-030-SS Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycolac® EX39F ABS Highest impact extrusion ABS for sheet and blow molding applications. FDA food contact compliant. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Europe-Africa-Middle East) High flow PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® XHT1141 PC XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP DL0029E PC (Europe-Africa-Middle East) LNP* Lubricomp* DL0029E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0090 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0090 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0090 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0090 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0090 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID GP2330BL PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Radiator Tank, Reservoir)Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0090 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® SG5500 PBT+PET+GF50% Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | Test Condition: 150x105x3; acc. ISO 2577 |
Ineos ABS Lustran® ABS M406 Lustran® ABS M406 has very high impact strength and increased chemical and dynamic resistance. It is used for the production of molded plastic articles. |
|||
Linear Mold Shrinkage, Flow | 0.0065 - 0.0090 cm/cm | 0.0065 - 0.0090 in/in | |
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm @Time 86400 sec |
0.0060 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 4012G PBT VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0080 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP RFB71S PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RFB71S is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Europe-Africa-Middle East) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF13-66 XE-NBK1 13% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | ISO DIS 294-4 |
Wellman Wellamid® MR410 42H-NBK1 40% Mineral Reinforced Nylon 6 Description: Mineral Reinforced Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | b.o. ISO 2577 |
Covestro Makroblend® UT5207 PC/PBT Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•.. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | on Tensile Bar; E2P method |
Eurostar Staramide ALY540A PA66, Glass/Mineral Fiber Reinforced, Injection Molding Staramide ALY540A is a Glass Fiber Reinforced, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0070 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycolac® EX39 ABS Highest impact extrusion ABS for sheet and blow molding applications. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOTUF VX99810 Super Tough Nylon Super Tough Nylon, Proprietary Filler(s), |