Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0065 cm/cm
0.0065 in/in
Polycasa Acryl® KR 2007/1 Acrylic
Medium stiffness impact grade with good heat distortion resistance. Can be extruded to thin tubes and profile and film. Easy to vacuum form. Lamp covers, cable boxes.Data was collected by ISO met..
Linear Mold Shrinkage, Flow 0.0065 cm/cm
0.0065 in/in
Polycasa Acryl® G 88 E Acrylic
Same as Lucryl G 88, but higher resistance to stress cracking and higher processing viscosity. Used for: extruded protective layer on PVC, ABS and PC for outdoor applications, as well as bath tubs ..
Linear Mold Shrinkage, Flow 0.0065 cm/cm
0.0065 in/in
Polycasa Acryl® KR 2006/1 Acrylic, Impact Grade
Impact-modified grade for highly stressed parts; highest impact and notched-impact resistance; can be mixed with general-purpose grades to get the desired toughness; highly resistant to stress crack..
Linear Mold Shrinkage, Flow 0.0065 cm/cm
0.0065 in/in
Polycasa Acryl® KR 2010/1 Acrylic, Impact Grade
High-impact grade with good flowability (e.g. for lamp covers).Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.
Linear Mold Shrinkage, Flow 0.0065 cm/cm
0.0065 in/in
Compression molding; ISO 2577
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed  (discontinued **)
Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications..
Linear Mold Shrinkage, Flow 0.0065 cm/cm
0.0065 in/in
Compression molding; ISO 2577
Hexion Bakelite™ PF 38110 Phenolic Formaldehyde Resin, High Surface Quality  (discontinued **)
Phenolic molding compound, mainly organically filled.Application areas: Devices for the electrical installation, pan handles, knobs, mainly for compression molding.Information provided by Bak AGBak ..
Linear Mold Shrinkage, Flow 0.0065 - 0.0085 cm/cm
0.0065 - 0.0085 in/in
LATI Latamid 12 CP/85 PA 12
Polyamide 12 (PA12) based compound. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Linear Mold Shrinkage, Flow 0.0065 - 0.0085 cm/cm
0.0065 - 0.0085 in/in
LATI Latishield 36/SP-05A ABS, Steel Fiber Reinforced
EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid..
Linear Mold Shrinkage, Flow 0.0065 cm/cm
0.0065 in/in
Solvay TECHNYL® C 52G1 V25 Grey R7035 (XC 1329/A) PA6, DRY
Description: Polyamide 6, Glass-filled, glow-wire modified, color stabilized, lubricated for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Application..
Linear Mold Shrinkage, Flow 0.0065 - 0.0073 cm/cm

@Thickness 3.20 mm
0.0065 - 0.0073 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Europe-Africa-Middle East)
PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Linear Mold Shrinkage, Flow 0.0065 - 0.0075 cm/cm

@Thickness 3.20 mm
0.0065 - 0.0075 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Europe-Africa-Middle East)
Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta..
Linear Mold Shrinkage, Flow 0.0065 cm/cm
0.0065 in/in
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Time 86400 sec
0.0065 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon DS0029 PC
LNP STAT-KON* DS0029 is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for t..
Linear Mold Shrinkage, Flow 0.0065 - 0.0073 cm/cm

@Thickness 3.20 mm
0.0065 - 0.0073 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific)
PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.0065 - 0.0075 cm/cm

@Thickness 3.20 mm
0.0065 - 0.0075 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® X5410 PC+PET
Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta..
Linear Mold Shrinkage, Flow 0.0065 cm/cm
0.0065 in/in
ISO 294-4,2577
Suzhou Hipro Polymers Hiprolon® 400 MC HLS G30 Nylon, 30% glass fiber filled
Hiprolon® 400 MC HLS G30 is a specialty long chain polyamide compound reinforced with 30% chopped glass fiber for injection molding. It contains some bio-renewable resources Features: high dime..
Linear Mold Shrinkage, Flow 0.0065 - 0.0105 cm/cm
0.0065 - 0.0105 in/in
ISO DIS 294-4
Wellman Wellamid® GF1811-BK1 15% Glass Fiber Reinforced Nylon 66
Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.0065 cm/cm
0.0065 in/in
b.o. ISO 2577
Covestro Makroblend® UT305 PC/PET Blend
Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• High moisture en..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Thickness 2.00 mm
0.0065 in/in

@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Covestro Makrolon® 1881 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Thickness 2.00 mm
0.0065 in/in

@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Covestro Makrolon® 1952 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Thickness 2.00 mm
0.0065 in/in

@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Covestro Makrolon® 2405 MAS048 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Thickness 2.00 mm
0.0065 in/in

@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Covestro Makrolon® 2405 MAS057 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Thickness 2.00 mm
0.0065 in/in

@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Covestro Makrolon® 2407 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Thickness 2.00 mm
0.0065 in/in

@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Covestro Makrolon® 2408 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Thickness 2.00 mm
0.0065 in/in

@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Covestro Makrolon® 2600 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Thickness 2.00 mm
0.0065 in/in

@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Covestro Makrolon® 2652 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Thickness 2.00 mm
0.0065 in/in

@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Covestro Makrolon® 2805 MAS152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Linear Mold Shrinkage, Flow 0.0065 cm/cm

@Thickness 2.00 mm
0.0065 in/in

@Thickness 0.0787 in
60x60x2 mm; 500 bar; ISO 294-4
Covestro Makrolon® FU1007 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications..
Linear Mold Shrinkage, Flow 0.0065 cm/cm
0.0065 in/in
ISO 294-4
DSM EcoPaXX® Q-HGM24 PA410-(GF+MD)30
10% Glass Reinforced, 20% Mineral Reinforced, Heat Stabilized
Linear Mold Shrinkage, Flow 0.0065 - 0.0105 cm/cm
0.0065 - 0.0105 in/in
LATI Latilub 88/50-30GRT PEEK, Graphite/PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Copyright © lookpolymers.com All Rights Reserved