Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0020 cm/cm | 0.0015 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ AS-15CF/000 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ CTX-1125 Natural Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ NN-30CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | ASTM D955 |
PolyOne Trilliant™ HC HC7300-0013 ESD Black Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 3414R PC (Asia Pacific) 40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
Ravago Manufacturing Americas Hylex® P1010G40 HB Polycarbonate, 40% Fiberglass Reinforced Information provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Edgetek® PC-15CF/000 FCR Polycarbonate (PC) The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Nymax™ GF 1200 60 HS Black 22 Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Nymax™ GF 1200 A 55 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0020 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOS GP2305A SAN+GF30%, General Purpose Feature: Injection Molding, SAN+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | |
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | |
LATI Larton L K/20 L-PPS, 20% Carbon Fiber Reinforced Linear Polyphenylene Sulfide (L-PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | |
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Time 86400 sec |
0.0010 - 0.0020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36F PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCP36F is a compound based on PPS - Linear resin containing Bearing Grade, Carbon Fiber, Lubricants. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON UEF26AS PPA (Europe-Africa-Middle East) LNP* Stat-kon* UEF26AS is a compound based on Polyphthalamide resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm @Time 86400 sec |
0.00050 - 0.0020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific) LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Time 86400 sec |
0.0010 - 0.0020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI LNP* THERMOCOMP* ECF62 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Time 86400 sec |
0.0010 - 0.0020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI (Asia Pacific) LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0018 - 0.0020 cm/cm @Time 86400 sec |
0.0018 - 0.0020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP QF00A PA6.10 LNP* THERMOCOMP* QF00A is a compound based on Nylon 6/10 containing 50% Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP RC003 PA 66 (Europe-Africa-Middle East) 15% carbon fibre reinforced Polyamide 66 injection moulding resin. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; ISO 294 |
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; E2P method |
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; E2P method |
Eurostar Starpylen MF007AS PP, Glass Fiber Filled, Injection Molded Starpylen MF007AS is a Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ISO 294-4 |
Polyplastic Armamid® PA6 GF 30 HS-901 Nylon, 30% Glass Filled Injection molding, heat stabilizedInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
Ravago Manufacturing Americas Hylex® P1310G40 HB Polycarbonate, 40% Fiberglass Reinforced, UV Stabilized Information provided by Ravago. |