Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | ASTM D955 |
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 78.6 MPa | 11400 psi | ASTM D638 |
Elongation at Break | 1.5 % | 1.5 % | Type I, 5.1 mm/min; ASTM D638 |
Tensile Modulus | 7.72 GPa | 1120 ksi | Type I, 5.1 mm/min; ASTM D638 |
Flexural Strength | 123 MPa | 17800 psi | ASTM D790 |
Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
Izod Impact, Notched | 0.430 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.806 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 6.35 mm |
216 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 97.0 °C @Thickness 6.35 mm |
207 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
Flammability, UL94 | HB | HB | Internal Method |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1000 ohm-cm - 1e+05 | 1000 ohm-cm - 1e+05 | ASTM D257 |
Surface Resistance | 1000 ohm - 1e+05 | 1000 ohm - 1e+05 | ASTM D257 |
Static Decay | 0.0020 sec | 0.0020 sec | (Mil-B-81705C), 12% RH, 5000 kV to 50 kV |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 227 - 238 °C | 441 - 460 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Features | Antistatic | |
Conductive | ||
Electrically Conductive | ||
Statically Conductive | ||
Filler / Reinforcement | Carbon Fiber Reinforcement, 13% Filler by Weight | |
Forms | Pellets | |
Generic Material | ABS | |
Generic Name | Acrylonitrile Butadiene Styrene (ABS) | |
Processing Method | Injection Molding | |
Regional Availability | Africa & Middle East | |
Asia Pacific | ||
Europe | ||
North America | ||
South America | ||
RoHS Compliance | RoHS Compliant | |
Uses | Computer Components | |
Connectors | ||
Electrical Housing | ||
Electrical/Electronic Applications | ||
Housings | ||
Medical Device Housings | ||
Medical/Healthcare Applications |