Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | ASTM D955 |
PolyOne LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | ASTM D955 |
PolyOne LubriOne™ AT-000/15T Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | ASTM D955 |
PolyOne LubriOne™ AT-000/20T Black Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Shell Carilon® DP R1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1000 is a high flow developmental engineering polyketone resin from Shell Chemi.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | |
LATI Latistat 73/13-06 POM Dissipative product based on Polyoxymethylene (POM). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP PL002 PA 6 LNP* LUBRICOMP* PL002 is a compound based on Nylon 6 base resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP QL004 PA6.10 LNP* LUBRICOMP* QL004 is a compound based on Nylon 6/10 containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RX99518 PA 66 LNP* LUBRICOMP* RX99518 is a compound based on PA66 containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WL002 PBT LNP* LUBRICOMP WL002 is a compound based on PBT resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66 LNP* LUBRILOY* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON FX98501 PE LNP* STAT-KON* FX98501 is a compound based on Polyethylene resin containing Proprietary Fillers. Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON WS002I PBT LNP* STAT-KON* WS002I is a compound based on PBT resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, High Impact. |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP MX95318 PP LNP* THERMOCOMP* MX95318 is a compound based on Polypropylene containing Proprietary Filler(s). |
|||
Linear Mold Shrinkage, Flow | >= 0.020 cm/cm @Time 86400 sec |
>= 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP WX05505 PBT LNP* Thermocomp* WX05505 is a compound based on Thermoplastic Polyester (PBT) resin containing proprietary fillers. |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | |
Solvay TECHNYL® A 208F PA66, DRY Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta.. |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm @Thickness 3.17 mm |
0.020 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® POM CO TL20 LE Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction, Low Extractables and CopolymerUL File Number: E.. |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | DAM; ISO 294-4 |
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Clariant PA233 Nylon 6, Improved Processability, Easily Colorable, Toughened Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Clariant Renol PBT1100TF10 Polybutylene Terephthalate, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | Eurotec |
Eurotec® Tecoform® PO20 NL RW POM, surface modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
Barlog Plastics KEBAFORM C 90 W POM Copolymer unreinforced, drinking water approved POMInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 2577 |
BASF Ultraform® W2320 U03 POM Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | Sim. To ISO 294-4 |
DSM Arnite® T06 204 XL PBT Low Viscosity, Injection Molding, Low outgassing |
|||
Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | Sim. To ISO 294-4 |
DSM Stanyl® TE300 PA46 Heat Stabilized |