Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible C9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Hytrel® 5553FG NC010 TPC-ET
(Unverified Data**) Hytrel® 5553FG NC010 is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm @Thickness 3.20 mm |
0.014 - 0.018 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI1202A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294 |
Inno-Comp INNOPOL® CS 2-3000 Polypropylene Block-Copolymer INNOPOL® CS 2-3000 is a polypropylene block-copolymer compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-3000 is developed for producing injection molded automot.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294 |
Inno-Comp INNOPOL® CS 2-5000 Polypropylene Block-Copolymer INNOPOL® CS 2-5000 is a polypropylene block-copolymer compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-5000 is developed for producing injection molded automot.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4, 2577 |
Kuraray Genestarâ„¢ N1001A-M41 Nylon Low friction unreinforced injection grade. Main Features:Low friction coefficientHigh impact strengthExamples of applications are:Friction and wear applicationGear and wheel |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4, 2577 |
Kuraray Genestarâ„¢ N1006A-M41 Nylon Impact modified unreinforced injection grade. Main Features:High elongationHigh impact strengthExamples of applications are:Retainers for quick connectorFlexible band |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers CPP-110 Polypropylene Homopolymer, 10% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | 60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | |
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | |
Solvay TECHNYL® A 218 S40 Black 21 N PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 218 S40 is used in all sectors of ind.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Time 86400 sec |
0.014 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON MD000AP PP LNP* STAT-KON* MD000AP is a compound based on Polypropylene containing Carbon Powder. Added features of this grade include: Electrically Conductive, Exceptional Processing. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP IB008 PA 6/12 (Europe-Africa-Middle East) LNP* Thermocomp* IB008 is a compound based on Nylon 6/12 resin containing Glass Bead. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Plastiblend® PA6 NAT001 Nylon 6 Availability: North AmericaForms: PelletsFeatures: Good Processability and High FlowAppearance: NaturalTPCI# 1327102Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 3.17 mm |
0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Plastiblend® PA6/6,6 L N Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and LubricantFeatures: Copolymer, Fast Molding Cycle, Nucleated and LubricatedProcessing Method: Injection MoldingInformation prov.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm @Thickness 3.20 mm |
0.014 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | 24Hr; ISO 294 3/4 |
CTC SunPro® SP 200 P 3085 Polypropylene Copolymer SunPro® SP 200 P 3085 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM.PP... |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSM-30/4 PA666-MD30 Information provided by EMS Grivory |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66
(Unverified Data**) Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® FG42L NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | Eurotec |
Eurotec® Tecomid® NB40 NL IM PA6, impact modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® 6646 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 66 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-30 MS Polyamide 6 - Natural High viscosity extrusion grade for blown and flat films, including biaxial oriented films, also for extrusion of rods, pipes, plates, sheets, low diameter tubes and for injection molding of thick-wa.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Diameter 2.00 mm |
0.014 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
Linear Mold Shrinkage, Flow | 0.014 cm/cm @Diameter 2.00 mm |
0.014 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, Conditioned Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |