| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | DAM; ISO 1183 |
| Water Absorption | 2.7 % <br>@Temperature 23.0 °C |
2.7 % <br>@Temperature 73.4 °F |
Equilibrium 50%RH; DAM; ISO 62, Similar to |
| 8.5 % <br>@Temperature 23.0 °C |
8.5 % <br>@Temperature 73.4 °F |
Saturation, immersed; DAM; ISO 62, Similar to | |
| Viscosity | 109000 cP <br>@Shear Rate 7000 1/s,<br> Temperature 305 °C |
109000 cP <br>@Shear Rate 7000 1/s,<br> Temperature 581 °F |
DAM; ISO 11443 |
| 119000 cP <br>@Shear Rate 7000 1/s,<br> Temperature 295 °C |
119000 cP <br>@Shear Rate 7000 1/s,<br> Temperature 563 °F |
DAM; ISO 11443 | |
| 136000 cP <br>@Shear Rate 5000 1/s,<br> Temperature 305 °C |
136000 cP <br>@Shear Rate 5000 1/s,<br> Temperature 581 °F |
DAM; ISO 11443 | |
| 144000 cP <br>@Shear Rate 7000 1/s,<br> Temperature 275 °C |
144000 cP <br>@Shear Rate 7000 1/s,<br> Temperature 527 °F |
DAM; ISO 11443 | |
| 150000 cP <br>@Shear Rate 5000 1/s,<br> Temperature 295 °C |
150000 cP <br>@Shear Rate 5000 1/s,<br> Temperature 563 °F |
DAM; ISO 11443 | |
| 182000 cP <br>@Shear Rate 5000 1/s,<br> Temperature 275 °C |
182000 cP <br>@Shear Rate 5000 1/s,<br> Temperature 527 °F |
DAM; ISO 11443 | |
| 243000 cP <br>@Shear Rate 2000 1/s,<br> Temperature 305 °C |
243000 cP <br>@Shear Rate 2000 1/s,<br> Temperature 581 °F |
DAM; ISO 11443 | |
| 274000 cP <br>@Shear Rate 2000 1/s,<br> Temperature 295 °C |
274000 cP <br>@Shear Rate 2000 1/s,<br> Temperature 563 °F |
DAM; ISO 11443 | |
| 342000 cP <br>@Shear Rate 2000 1/s,<br> Temperature 275 °C |
342000 cP <br>@Shear Rate 2000 1/s,<br> Temperature 527 °F |
DAM; ISO 11443 | |
| 360000 cP <br>@Shear Rate 1000 1/s,<br> Temperature 305 °C |
360000 cP <br>@Shear Rate 1000 1/s,<br> Temperature 581 °F |
DAM; ISO 11443 | |
| 413000 cP <br>@Shear Rate 1000 1/s,<br> Temperature 295 °C |
413000 cP <br>@Shear Rate 1000 1/s,<br> Temperature 563 °F |
DAM; ISO 11443 | |
| 431000 cP <br>@Shear Rate 700 1/s,<br> Temperature 305 °C |
431000 cP <br>@Shear Rate 700 1/s,<br> Temperature 581 °F |
DAM; ISO 11443 | |
| 501000 cP <br>@Shear Rate 700 1/s,<br> Temperature 295 °C |
501000 cP <br>@Shear Rate 700 1/s,<br> Temperature 563 °F |
DAM; ISO 11443 | |
| 504000 cP <br>@Shear Rate 500 1/s,<br> Temperature 305 °C |
504000 cP <br>@Shear Rate 500 1/s,<br> Temperature 581 °F |
DAM; ISO 11443 | |
| 535000 cP <br>@Shear Rate 1000 1/s,<br> Temperature 275 °C |
535000 cP <br>@Shear Rate 1000 1/s,<br> Temperature 527 °F |
DAM; ISO 11443 | |
| 593000 cP <br>@Shear Rate 500 1/s,<br> Temperature 295 °C |
593000 cP <br>@Shear Rate 500 1/s,<br> Temperature 563 °F |
DAM; ISO 11443 | |
| 664000 cP <br>@Shear Rate 700 1/s,<br> Temperature 275 °C |
664000 cP <br>@Shear Rate 700 1/s,<br> Temperature 527 °F |
DAM; ISO 11443 | |
| 806000 cP <br>@Shear Rate 500 1/s,<br> Temperature 275 °C |
806000 cP <br>@Shear Rate 500 1/s,<br> Temperature 527 °F |
DAM; ISO 11443 | |
| Linear Mold Shrinkage, Flow | 0.014 cm/cm <br>@Thickness 2.00 mm |
0.014 in/in <br>@Thickness 0.0787 in |
DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.014 cm/cm <br>@Thickness 2.00 mm |
0.014 in/in <br>@Thickness 0.0787 in |
DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Stress | 13.4 MPa <br>@Strain 3.00 %,<br> Temperature 90.0 °C |
1940 psi <br>@Strain 3.00 %,<br> Temperature 194 °F |
50%RH; ISO 527 |
| 14.5 MPa <br>@Strain 5.00 %,<br> Temperature 120 °C |
2100 psi <br>@Strain 5.00 %,<br> Temperature 248 °F |
50%RH; ISO 527 | |
| 15.9 MPa <br>@Strain 3.00 %,<br> Temperature 60.0 °C |
2310 psi <br>@Strain 3.00 %,<br> Temperature 140 °F |
50%RH; ISO 527 | |
| 17.6 MPa <br>@Strain 5.00 %,<br> Temperature 120 °C |
2550 psi <br>@Strain 5.00 %,<br> Temperature 248 °F |
DAM; ISO 527 | |
| 19.7 MPa <br>@Strain 3.00 %,<br> Temperature 40.0 °C |
2860 psi <br>@Strain 3.00 %,<br> Temperature 104 °F |
50%RH; ISO 527 | |
| 20.9 MPa <br>@Strain 10.0 %,<br> Temperature 120 °C |
3030 psi <br>@Strain 10.0 %,<br> Temperature 248 °F |
50%RH; ISO 527 | |
| 21.1 MPa <br>@Strain 6.00 %,<br> Temperature 90.0 °C |
3060 psi <br>@Strain 6.00 %,<br> Temperature 194 °F |
50%RH; ISO 527 | |
| 21.8 MPa <br>@Strain 5.00 %,<br> Temperature 90.0 °C |
3160 psi <br>@Strain 5.00 %,<br> Temperature 194 °F |
DAM; ISO 527 | |
| 22.4 MPa <br>@Strain 0.800 %,<br> Temperature 40.0 °C |
3250 psi <br>@Strain 0.800 %,<br> Temperature 104 °F |
DAM; ISO 527 | |
| 23.5 MPa <br>@Strain 10.0 %,<br> Temperature 120 °C |
3410 psi <br>@Strain 10.0 %,<br> Temperature 248 °F |
DAM; ISO 527 | |
| 24.2 MPa <br>@Strain 15.0 %,<br> Temperature 120 °C |
3510 psi <br>@Strain 15.0 %,<br> Temperature 248 °F |
50%RH; ISO 527 | |
| 24.8 MPa <br>@Strain 6.00 %,<br> Temperature 60.0 °C |
3600 psi <br>@Strain 6.00 %,<br> Temperature 140 °F |
50%RH; ISO 527 | |
| 24.9 MPa <br>@Strain 0.800 %,<br> Temperature 23.0 °C |
3610 psi <br>@Strain 0.800 %,<br> Temperature 73.4 °F |
DAM; ISO 527 | |
| 25.8 MPa <br>@Strain 9.00 %,<br> Temperature 90.0 °C |
3740 psi <br>@Strain 9.00 %,<br> Temperature 194 °F |
50%RH; ISO 527 | |
| 26.1 MPa <br>@Strain 20.0 %,<br> Temperature 120 °C |
3790 psi <br>@Strain 20.0 %,<br> Temperature 248 °F |
50%RH; ISO 527 | |
| 26.3 MPa <br>@Strain 15.0 %,<br> Temperature 120 °C |
3810 psi <br>@Strain 15.0 %,<br> Temperature 248 °F |
DAM; ISO 527 | |
| 27.2 MPa <br>@Strain 25.0 %,<br> Temperature 120 °C |
3950 psi <br>@Strain 25.0 %,<br> Temperature 248 °F |
50%RH; ISO 527 | |
| 27.2 MPa <br>@Strain 3.00 %,<br> Temperature 60.0 °C |
3950 psi <br>@Strain 3.00 %,<br> Temperature 140 °F |
DAM; ISO 527 | |
| 27.9 MPa <br>@Strain 30.0 %,<br> Temperature 120 °C |
4050 psi <br>@Strain 30.0 %,<br> Temperature 248 °F |
50%RH; ISO 527 | |
| 27.9 MPa <br>@Strain 20.0 %,<br> Temperature 120 °C |
4050 psi <br>@Strain 20.0 %,<br> Temperature 248 °F |
DAM; ISO 527 | |
| 28.2 MPa <br>@Strain 35.0 %,<br> Temperature 120 °C |
4090 psi <br>@Strain 35.0 %,<br> Temperature 248 °F |
50%RH; ISO 527 | |
| 28.3 MPa <br>@Strain 40.0 %,<br> Temperature 120 °C |
4100 psi <br>@Strain 40.0 %,<br> Temperature 248 °F |
50%RH; ISO 527 | |
| 28.4 MPa <br>@Strain 45.0 %,<br> Temperature 120 °C |
4120 psi <br>@Strain 45.0 %,<br> Temperature 248 °F |
50%RH; ISO 527 | |
| 28.5 MPa <br>@Strain 50.0 %,<br> Temperature 120 °C |
4130 psi <br>@Strain 50.0 %,<br> Temperature 248 °F |
50%RH; ISO 527 | |
| 28.5 MPa <br>@Strain 3.00 %,<br> Temperature 23.0 °C |
4130 psi <br>@Strain 3.00 %,<br> Temperature 73.4 °F |
50%RH; ISO 527 | |
| 28.8 MPa <br>@Strain 12.0 %,<br> Temperature 90.0 °C |
4180 psi <br>@Strain 12.0 %,<br> Temperature 194 °F |
50%RH; ISO 527 | |
| 28.9 MPa <br>@Strain 25.0 %,<br> Temperature 120 °C |
4190 psi <br>@Strain 25.0 %,<br> Temperature 248 °F |
DAM; ISO 527 | |
| 29.6 MPa <br>@Strain 30.0 %,<br> Temperature 120 °C |
4290 psi <br>@Strain 30.0 %,<br> Temperature 248 °F |
DAM; ISO 527 | |
| 29.6 MPa <br>@Strain 10.0 %,<br> Temperature 90.0 °C |
4290 psi <br>@Strain 10.0 %,<br> Temperature 194 °F |
DAM; ISO 527 | |
| 30.0 MPa <br>@Strain 35.0 %,<br> Temperature 120 °C |
4350 psi <br>@Strain 35.0 %,<br> Temperature 248 °F |
DAM; ISO 527 | |
| 30.1 MPa <br>@Strain 6.00 %,<br> Temperature 40.0 °C |
4370 psi <br>@Strain 6.00 %,<br> Temperature 104 °F |
50%RH; ISO 527 | |
| 30.3 MPa <br>@Strain 9.00 %,<br> Temperature 60.0 °C |
4390 psi <br>@Strain 9.00 %,<br> Temperature 140 °F |
50%RH; ISO 527 | |
| 30.4 MPa <br>@Strain 40.0 %,<br> Temperature 120 °C |
4410 psi <br>@Strain 40.0 %,<br> Temperature 248 °F |
DAM; ISO 527 | |
| 30.6 MPa <br>@Strain 45.0 %,<br> Temperature 120 °C |
4440 psi <br>@Strain 45.0 %,<br> Temperature 248 °F |
DAM; ISO 527 | |
| 30.7 MPa <br>@Strain 15.0 %,<br> Temperature 90.0 °C |
4450 psi <br>@Strain 15.0 %,<br> Temperature 194 °F |
50%RH; ISO 527 | |
| 30.7 MPa <br>@Strain 50.0 %,<br> Temperature 120 °C |
4450 psi <br>@Strain 50.0 %,<br> Temperature 248 °F |
DAM; ISO 527 | |
| 31.9 MPa <br>@Strain 18.0 %,<br> Temperature 90.0 °C |
4630 psi <br>@Strain 18.0 %,<br> Temperature 194 °F |
50%RH; ISO 527 | |
| 32.7 MPa <br>@Strain 21.0 %,<br> Temperature 90.0 °C |
4740 psi <br>@Strain 21.0 %,<br> Temperature 194 °F |
50%RH; ISO 527 | |
| 33.1 MPa <br>@Strain 24.0 %,<br> Temperature 90.0 °C |
4800 psi <br>@Strain 24.0 %,<br> Temperature 194 °F |
50%RH; ISO 527 | |
| 33.3 MPa <br>@Strain 27.0 %,<br> Temperature 90.0 °C |
4830 psi <br>@Strain 27.0 %,<br> Temperature 194 °F |
50%RH; ISO 527 | |
| 33.4 MPa <br>@Strain 30.0 %,<br> Temperature 90.0 °C |
4840 psi <br>@Strain 30.0 %,<br> Temperature 194 °F |
50%RH; ISO 527 |