Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Nucleated
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:BearingsCamsConnectorsFastenersGeneral PurposeHousingsIndustrial ApplicationsAppearance: Natural ColorForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 1.2 %
<br>@Time 86400 sec
1.2 %
<br>@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.4 %
2.4 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.014 cm/cm
<br>@Diameter 2.00 mm
0.014 in/in
<br>@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm
<br>@Diameter 2.00 mm
0.016 in/in
<br>@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527-2
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-2
Elongation at Break 20 %
20 %
ISO 527-2
Elongation at Yield 15 %
15 %
ISO 527-2
Tensile Modulus 2.50 GPa
363 ksi
ISO 527-2
Flexural Strength 35.0 MPa
5080 psi
ISO 178
Flexural Modulus 1.30 GPa
189 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
<br>@Temperature -30.0 °C
2.38 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180
15.0 kJ/m²
<br>@Temperature 23.0 °C
7.14 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched NB
<br>@Temperature -30.0 °C
NB
<br>@Temperature -22.0 °F
ISO 179/1eU
NB
<br>@Temperature 23.0 °C
NB
<br>@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
<br>@Temperature -30.0 °C
2.38 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
1.50 J/cm²
<br>@Temperature 23.0 °C
7.14 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA