Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 925 PC (Asia Pacific) Lexan* 925 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating. Lexan resin 925 is available in various opa.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycolac® EX58 ABS High impact ABS for sheet extrusion and blow molding applications. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 6.40 mm |
0.0060 - 0.0080 in/in @Thickness 0.252 in |
SABIC Method |
SABIC Innovative Plastics Lexan® FL2000 PC Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Time 86400 sec |
0.0060 - 0.0080 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP COLORCOMP DX98550H PC LNP* COLORCOMP* DX98550H is an unfilled Polycarbonate resin. Added features of this grade are: Low Extractable, Healthcare. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | Test Condition: 150x105x3; acc. ISO 2577 |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4 |
Mitsubishi Xantar® 24 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers PC-1428 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | |
LATI Latamid 66 MDT03-01 PA 66 Polyamide 66 (PA66) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4 |
Mitsubishi Xantar® FC 19 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | |
Solvay TECHNYL® R AR 130/GF Nylon 66, 30% glass fiber, DRY Description: TECHNYL® AR 130/GF is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. It contains recycled raw materials. This product is available in bla.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® ABS 04001 BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Time 86400 sec |
0.0060 - 0.0080 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY D20009 PC (Asia Pacific) LNP LUBRILOY* D20009 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | |
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU) Veradel® 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, .. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF/B20 A3 BK 20% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: .. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Europe-Africa-Middle East) PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6/6 GF15 ML3 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: Natural ColorInformation provi.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Plastiblend® ABS 8011 Availability: North AmericaForms: PelletsFeatures: PlatableInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA 10% Glass Reinforced PPE+PA Alloy. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL PX2245 PPE+HIPS (Europe-Africa-Middle East) NORYL PX2245 is a halogen free (according to VDE/DIN 472 part815) flame retardant material. The material fulfills the IEC 65 part 20.2 requirement at 1.6 mm thickness. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | ISO 2577 |
Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Conditioned) Description: Terblend® N NG-02 EF is a glass fiber reinforced UV stabilized ABS/PA blend with excellent dimensional stability and high impact strength. The enhanced flowability enables excellent .. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | ISO DIS 294-4 |
Wellman Wellamid® MR410 22H-GY1 40% Mineral Reinforced Nylon 66 Description: Mineral Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D955 |
Clariant Renol PCSP0008BK Polycarbonate, ESD Protection Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | |
BASF Luranyl® KR 2460/3 Polyphenylene Ether + Styrene-Butadiene Blend Flame retardant grade with very high heat resistance; used for precision parts and where the material must withstand high injection temperatures (e.g. heater-fan impellers).Data was collected by ISO.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4 |
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Conditioned, 15% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm @Time 86400 sec |
0.0060 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP CL001I PS LNP* Lubricomp* CL001I is a compound based on Polystyrene resin containing 5% PTFE. Added features of this material include: Internally Lubricated, High Impact. |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL FN215Z PPE+HIPS (Asia Pacific) PPE + PS, FR foam molding grade |
|||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® ABS SLX2 MB Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |