| Category | Polymer , Thermoplastic , ABS Polymer | 
| Manufacturer | Techmer ES | 
| Trade Name | Plastiblend® | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Techmer ES Plastiblend® ABS 8011.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 | 
| Linear Mold Shrinkage, Flow | 0.0060           cm/cm @Thickness 3.17 mm | 0.0060           in/in @Thickness 0.125 in | ASTM D955 | 
| Melt Flow | 4.0           g/10 min @Load 3.80 kg, Temperature 230 °C | 4.0           g/10 min @Load 8.38 lb, Temperature 446 °F | ASTM D1238 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Rockwell R | 104 | 104 | ASTM D785 | 
| Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D638 | 
| Elongation at Break | 3.5 % | 3.5 % | ASTM D638 | 
| Flexural Strength | 76.5 MPa | 11100 psi | ASTM D790 | 
| Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D790 | 
| Izod Impact, Notched | 0.747           J/cm @Thickness 3.17 mm, Temperature -40.0 °C | 1.40           ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F | ASTM D256 | 
| 2.14           J/cm @Thickness 3.17 mm, Temperature 22.8 °C | 4.00           ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F | ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 219 °F | Unannealed; ASTM D648 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 | 
| Vicat Softening Point | 104 °C | 220 °F | Rate B (120°C/h); ASTM D1525 |