Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Conditioned)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced , Nylon
Manufacturer Styrolution
Trade Name Terblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Terblend® N NG-02 EF is a glass fiber reinforced UV stabilized ABS/PA blend with excellent dimensional stability and high impact strength. The enhanced flowability enables excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.3 %
1.3 %
23°C/50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ISO 2577
Melt Flow 44.8 g/10 min
<br>@Load 10.0 kg,<br> Temperature 240 °C
44.8 g/10 min
<br>@Load 22.0 lb,<br> Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Ball Indentation Hardness 62.0 MPa
<br>@Load 36.5 kg,<br> Time 30.0 sec
8990 psi
<br>@Load 80.5 lb,<br> Time 0.00833 hour
ISO 2039-1
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO 527-1/-2
Elongation at Break 12 %
12 %
Nominal, 50 mm/min; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
ISO 527-1/-2
Tensile Modulus 2.40 GPa
348 ksi
ISO 527-1/-2
Izod Impact, Notched (ISO) 5.00 kJ/m²
<br>@Temperature -30.0 °C
2.38 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180/A
25.0 kJ/m²
<br>@Temperature 23.0 °C
11.9 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched 3.50 J/cm²
<br>@Temperature -30.0 °C
16.7 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
8.00 J/cm²
<br>@Temperature 23.0 °C
38.1 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
<br>@Temperature -30.0 °C
2.86 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
2.50 J/cm²
<br>@Temperature 23.0 °C
11.9 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Vicat Softening Point 118 °C
244 °F
VST/B/50; ISO 306
200 °C
392 °F
VST/A/50; ISO 306
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Dielectric Constant 3.8
<br>@Frequency 1.00e+6 Hz
3.8
<br>@Frequency 1.00e+6 Hz
IEC 60250
Dissipation Factor 0.090
<br>@Frequency 1.00e+6 Hz
0.090
<br>@Frequency 1.00e+6 Hz
IEC 60250
Processing Properties Metric English Comments
Melt Temperature 240 - 270 °C
464 - 518 °F
Injection Molding
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Injection Molding
Descriptive Properties Value Comments
Color Natural
Commercial Status Europe