Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | ASTM D955 |
PolyOne Nymax™ MF 1200 A 40 HS Natural Polyamide 66 (Nylon 66) The Nymax® MF 1200 Series of mineral-reinforced nylon 6/6 compounds have been specifically engineered to provide an excellent balance of physical property performance, toughness, chemical resistanc.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | ASTM D955 |
PolyOne Edgetek® XT XT-500-CU00 Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX1619 PC Lexan* LUX1619 Polycarbonate resin is an extrusion grade. It is UL94 HB rated. It was designed for high light reflectance. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | ASTM D955 |
PolyOne Edgetek® XT XT-500-CX02 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.18 mm |
0.0080 - 0.010 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125"; ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI2202B(W) PA66+GF20%, High Impact Feature: Injection Molding, PA66+GF20%, High ImpactApplication: Automotive (Covers)CAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.010 cm/cm @Thickness 3.20 mm |
0.0050 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HF5254A PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL HI5302R PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.010 cm/cm @Thickness 3.20 mm |
0.0090 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL TE5108H PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.010 cm/cm @Thickness 3.20 mm |
0.0040 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP2300R PBT+GF30% Description: Injection Molding, PBT+GF30%, Anti-HydrolysisApplication: E&E (Speed Nut & Body)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.010 cm/cm @Thickness 3.20 mm |
0.0030 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | |
LATI Latamid 66 MDT03-01 PA 66 Polyamide 66 (PA66) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Linear Mold Shrinkage, Flow | 0.0075 - 0.010 cm/cm | 0.0075 - 0.010 in/in | |
LATI Latene® 7H2W T-V0 PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardantsAvailability: Africa & Middle East; Asia Pacif.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL GP3402 PP+MF40% Description: Injection Molding, PP+MF40%, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.010 cm/cm @Thickness 3.20 mm |
0.0090 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL TE5104 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | |
LATI Latimass 82-06 D030 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Time 86400 sec |
0.0080 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.010 cm/cm @Thickness 3.20 mm |
0.0040 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 815F PBT+PET PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Time 86400 sec |
0.0080 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX11408 PC LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 1103 PBT+PC AUTOMOTIVE. Unreinforced, impact modified PBT+PC alloy. Excellent low temperature impact and chemical resistance. Range gray, black colors. |
|||
Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics LNP Thermocomp MH0200A PP (Europe-Africa-Middle East) LNP* Thermocomp* MH0200A is a compound based on Polypropylene resin containing High Specific Gravity Filler.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | |
Solvay TECHNYL® 2417IG PA66, 20% glass fiber, DRY Description: Polyamide 66, 20% glass fiber reinforced, Impact modified for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2417IG4 is used in all sectors of industries,.. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | ASTM D955 |
Lubrizol Estane® 2103-65D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low temperature impactAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.010 cm/cm | 0.0050 - 0.010 in/in | ASTM D955 |
Clariant Renol PA2SP0010HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm @Thickness 3.20 mm |
0.0070 - 0.010 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |